Method of manufacturing a semiconductor device
Abstract
By using lasers having different wavelengths in laser annealing of an amorphous semiconductor film, the amorphous semiconductor film can be crystallized and the crystallinity of the crystallized film is improved. A laser 126 to 370 nm in wavelength is used first to subject an amorphous semiconductor film to laser annealing, thereby obtaining a crystalline semiconductor film. In desirable laser annealing, a subject surface is irradiated with a laser beam processed by an optical system into a linear laser beam that is linear in section on the subject surface. Next, a laser 370 to 650 nm in wavelength is used to irradiate the above crystalline semiconductor film by again processing the laser beam into a linear beam through an optical system. A crystalline semiconductor film thus obtained has an excellent crystallinity. If this crystalline semiconductor film is used to form an active layer of a TFT, an electric characteristic of the TFT can be improved.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 32.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of manufacturing a semiconductor device, comprising: forming an amorphous semiconductor film over a substrate; irradiating the amorphous semiconductor film with a first laser beam to form a first crystalline semiconductor film; and irradiating the first crystalline semiconductor film with a second laser beam to form a second crystalline semiconductor film, wherein the first laser beam is a third harmonic of a first YAG laser, and wherein the second laser beam is a second harmonic of a second YAG laser.
- Claim 2Depends on #1
A method according to claim 1 , wherein the first laser beam and the second laser beam are different in wavelength from each other.
- Claim 3Independent Claim
A method of manufacturing a semiconductor device, comprising: forming an amorphous semiconductor film over a substrate; irradiating the amorphous semiconductor film with a first laser beam to f
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 32 total)
References Cited — Backward Prior Art (50)
Non-Patent Literature (5)
- Bonnel, M. et al, "Polycrystalline Silicon Thin-Film Transistors with Two-Step Annealing Process," IEEE Electron Device Letters, vol. 14, No. 12, pp. 551-553, Dec., (1993).
- English abstract re Japanese Patent Application No. JP 10-092576, published Apr. 10, 1998.
- English abstract re Japanese Patent Application No. JP 7-130652, published May 19, 1995.
- Fujieda, I. et al, "Self-Referenced Poly-Si TFT Amplifier Readout for a Linear Image Sensor," IDEM 93, pp. 587-590, (1993).
- Fuse, M. et al, "Performance of Poly-Si Thin Film Transistors Fabricated by Excimer-Laser Annealing of SiH4<-> and Si2H6<-> Source Low Pressure Vapor Deposited a-Si Films With or Without Sold-Phase Crystallization," Solid State Phenomena, vols. 37-38, pp. 565-570 (1994).