Method for fabricating semiconductor device using photoresist pattern formed with argon fluoride laser
Abstract
The present invention provides a method for fabricating a semiconductor device with use of an ArF light source capable of minimizing deformations of a photoresist pattern for ArF during an etching process. Also, when forming the pattern, C 5 F 8 gas is used at a main etching step to compensate etch tolerance of the photoresist for ArF. By controlling process recipe properly, it is possible to minimize pattern deformations as simultaneously as to form a micronized pattern. To compensate the etch tolerance of the photoresist for ArF weaker than that of a photoresist for KrF, the main etching step is divided into three sub-steps, thereby providing a method for minimizing the pattern deformations when duplicating the pattern.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 11.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for fabricating a semiconductor device with use of an ArF light source, comprising the steps of: forming an etch stop layer and an insulating layer sequentially on a substrate; forming an anti-reflective coating layer on top of the insulating layer; forming a photoresist pattern on the anti-reflective coating layer by performing a photo-etching process using a photoresist and a ArF light source; exposing the insulating layer by etching the anti-reflective coating layer through the use of the photoresist pattern as an etch mask; etching selectively a partial portion of the exposed insu
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗