Method of preparing CRT funnel glass capable of effectively recycling another glass member
Abstract
A method for producing CRT funnel glass having a glass composition containing MgO, CaO, SrO, BaO and ZnO as essential components. Further, the total content of MgO, CaO, SrO, BaO and ZnO falls within a range of 5 to 13 mass %. As a glass material of the CRT funnel glass, CRT panel glass or CRT neck glass may be used. The method comprises preparing the glass material so as to contain MgO, CaO, SrO, BaO, and ZnO as essential components and so that the total content of MgO+CaO+SrO+BaO+ZnO falls within a range of 5 to 13 mass %; and melting the glass material.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 3.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of producing CRT funnel glass by using, as glass material, at least one of CRT panel glass and CRT neck glass, the method comprising the steps of: preparing the glass material so as to contain MgO, CaO, SrO, BaO, and ZnO as essential components and so that the total content of MgO+CaO+SrO+BaO+ZnO falls within a range of 5 to 13 mass %; and melting the glass material.
- Claim 2Depends on #1
The method according to claim 1 , wherein the preparing step is carried out so that the content of SrO and the content of BaO are each 1 mass % or greater.
- Claim 3Depends on #1
The method according to claim 1 , wherein the preparing step is carried out so that the CRT funnel glass has an alkali elution amount of 04 mg or less.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (3 of 3 total)
References Cited — Backward Prior Art (16)
Non-Patent Literature (1)
- European Search Report.