Boron carbide composite bodies, and methods for making same
Abstract
A composite body produced by a reactive infiltration process that possesses high mechanical strength, high hardness and high stiffness has applications in such diverse industries as precision equipment and ballistic armor. Specifically, the composite material features a boron carbide filler or reinforcement phase, and a silicon carbide matrix produced by the reactive infiltration of an infiltrant having a silicon component with a porous mass having a carbonaceous component. Potential deleterious reaction of the boron carbide with silicon during infiltration is suppressed by alloying or dissolving boron into the silicon prior to contact of the silicon infiltrant with the boron carbide. In a preferred embodiment of the invention related specifically to armor, good ballistic performance can be advanced by loading the porous mass or preform to be infiltrated to a high degree with one or more hard fillers such as boron carbide, and by limiting the size of the largest particles making up the mass. The instant reaction-bonded silicon carbide (RBSC) composite bodies surpass previous RBSC's as armor materials, and in this capacity approach the ballistic performance of current carbide ar
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 25 · Forward citations: 64.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A ballistic armor, comprising: at least one body having a front face and a rear face, the front face being the surface upon which a ballistic projectile impinges on said body, the body comprising a composite material having a hardness of at least about 1100 kg/mm 2 as measured with a Vickers indenter using a 1 kilogram load, the composite material further comprising (a) a matrix comprising silicon carbide crystallites, wherein at least about 90 volume percent of crystallites of said silicon carbide are smaller than about 100 microns in diameter; (b) at least 65 percent by volume of a reinforc
- Claim 2Depends on #1
The ballistic armor of claim 1 , wherein said at least one filler m
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 64 total)
References Cited — Backward Prior Art (25)
Non-Patent Literature (4)
- "Reaction-Bonded Silicon Carbide", Ceramics and Glasses Handbook, American Society for Materials, p. 293, 1990.
- D. ViechnickI, W. Blumenthal, M. Slavin, C. Tracy, and H. Skeele, "Armor Ceramics-1987", pp. 27-53, presented at Third TACOM Armor Coordinating Conference, Feb. 17-19, 1987, Monterey, California.
- Dennis J. ViechnickI, Michael J. Slavin and Morton I. KlIman, "Development and Current Status of Armor Ceramics", Ceramic Bulletin, vol. 70, No. 6, pp. 1035-1039 (1991).
- Roy C. Laible, "Ceramic Composite ArMOR", in Ballistic Materials and Penetration Mechanics, pp. 150-151, Elsevier Scientific Publishing Co., (1980).