Method of heat-treating nitride compound semiconductor layer and method of producing semiconductor device
Abstract
A method of heat-treating a nitride compound semiconductor layer, comprising heating a nitride compound semiconductor layer doped with a p-type impurity at a temperature that is at least 200° C. but less than 400° C. for at least 100 minutes.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 8.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of decreasing the resistance of and activating a nitride compound semiconductor layer doped with a p-type impurity, said method comprising heating a nitride compound semiconductor layer doped with a p-type impurity, at a temperature that is at least 200° C. but less than 400° C. for at least 200 minutes, in one atmosphere selected from; (A) aerial atmosphere, (B) an atmosphere supplied with an oxygen gas and a hydrogen gas, (C) an atmosphere supplied with an oxygen gas and steam, (D) an atmosphere supplied with an oxygen gas, a hydrogen gas and steam, (E) an inert gas atmosphere conta
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (8 of 8 total)
References Cited — Backward Prior Art (14)
Non-Patent Literature (2)
- The '662 patent claims priority from ref. AG as filed.
- The '678 patent claims priority from ref. AG as filed.