US 6,858,060 B2#26609044 Most CitedExpiredUnited States (USPTO)Utility

Process for the production of composite components by powder injection molding, and composite powders suitable for this purpose

4Forward Citations (#26609044 Global)
0.2/yrCitation Velocity (#34871386 Global)
1.18Citation PageRank (#32967172 Global)
20Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The invention relates to a process for the production of metallic and metal-ceramic composite components by powder injection molding of a system comprising a metal composite powder, a binder and optionally a ceramic component, where the metal composite powder used is mixed with a protecting liquid in an inert atmosphere before the mixing with the binder. The invention furthermore relates to molybdenum/copper and tungsten/copper composite powders which have a primary metal particle size of predominantly <2 μm, an oxygen content of <0.8% by weight and optionally a ceramic component, to the use of these composite powders for the production of composite components by powder injection molding, and to a process for the preparation of composite powders in which oxides of molybdenum or tungsten and of copper are mixed, dry-ground and reduced using hydrogen at a temperature of from 800 to 1050° C., and a ceramic component is optionally admixed with the resultant metal composite powder.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 4.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for forming a molybdenum/copper composite powder comprising a primary metal particle size of predominantly less than about 2 μm and an oxygen content of less than about 0.8% by weight, the process comprising: (a) mixing oxides of molybdenum and of copper and forming a mixture, and (b) dry-grinding and reducing the mixture with dry hydrogen at a temperature ranging from about 800 to about 1050° C. and forming the composite powder.

  2. Claim 2Independent Claim

    A process for forming a tungsten/copper composite powder, wherein it has a primary metal particle size of predominantly less than about 2 μm and an oxygen content of less than about 0.8% by weight, the process comprising: (a) mixing oxides of tungsten and of copper and forming a mixture, (b) dry-grinding and reducing the mixture with dry hydrogen at a temperature of from about 800 to about 1050° C. and forming the c

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (20)

PatentTitleYearCitations
US 3,418,103 AProcess for making tungsten and molybdenum alloys196816
US 3,652,746 AProcess for producing metal powder containing iron and molybdenum19723
JP S5321014 APreserving method for powder of metal or alloy—3
US 4,498,395 APowder comprising coated tungsten grains198563
US 4,915,733 AAgglomerated metal composite powders199051
US 4,915,733 B1Agglomerated metal composite powders199351
US 5,314,658 AConditioning metal powder for injection molding199420
US 5,468,457 AMethod of making tungsten-copper composite oxides19959
US 5,470,549 AMethod of making tungsten-copper composite oxides199517
EP 0,753,592 A1Copper-tungsten alloys and process for producing the same—5
US 5,641,920 APowder and binder systems for use in powder molding199768
US 5,686,676 AProcess for making improved copper/tungsten composites199731
US 5,889,220 ACopper-tungsten alloys and their manufacturing methods199919
US 5,905,938 AMethod of manufacturing a semiconductor substrate material19997
US 5,950,063 AMethod of powder injection molding199991
US 5,956,560 ATungsten-copper composite powder199920
US 5,993,731 AProcess for making improved net shape or near net shape metal parts199924
US 6,103,392 ATungsten-copper composite powder200030
DE 19,962,015 A1Compound powder mixtures used, e.g., for particle blasting, are produced using one powder type of a metal with a high melting point, hard material or ceramic together with a bonding metal—6
US 2001041146 A1Method for producing powder compact and method for manufacturing magnet—13

Non-Patent Literature (1)

  • Database WPI, Section Ch, Week 7815 Derwent Publications Ltd., London, GB; Class L, p. 03, AN 1978-27489A[15] XP002188188 & JP 53 021014 A (TDK Electronics Co Ltd), Feb. 27, 1978 Zusammenfassung.