US 6,855,229 B2#5954860 Most CitedExpiredUnited States (USPTO)Utility

Low viscosity bilayer disrupted softening composition for tissue paper

16Forward Citations (#5954860 Global)
0.8/yrCitation Velocity (#9816410 Global)
1.88Citation PageRank (#15984483 Global)
50Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Disclosed is a composition for softening a wet laid cellulosic structure. A particularly preferred structure is an absorbent tissue. Further disclosed are tissue structures softened using the composition. The composition includes an effective amount of a softening active ingredient; a vehicle in which the softening active ingredient is dispersed; an electrolyte dissolved in the vehicle; and a bilayer disrupter. The electrolyte and the bilayer disrupter cooperate to cause the viscosity of the composition to be less than the viscosity of a dispersion of the softening active ingredient in the vehicle alone. Preferably, the softening active ingredient is a quaternary ammonium compound with the formula: (R 1 ) 4-m —N + —[(CH 2 ) n —Y—R 3 ] m X − the vehicle is water, the electrolyte is calcium chloride, and the bilayer disrupter is a nonionic surfactant. Also disclosed is a method of using the compound by adding it at a use concentration to the wet end of a papermaking process.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 16.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of producing a soft tissue paper product, the method comprising the steps of: a) providing a chemical softening composition, said chemical softening composition comprising: a vehicle; a softening active ingredient, wherein said softening active ingredient comprises a quaternary ammonium compound; an electrolyte; and a bilayer disrupter; b) diluting said chemical softening composition to a use concentration; c) providing a slurry of papermaking fibers; d) treating said slurry of papermaking fibers with said diluted chemical softening composition; e) depositing said treated slurry of sa

  2. Claim 2Depends on #1

    The method of claim 1 wherein said method comprises the additional steps of

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,301,746 AProcess for forming absorbent paper by imprinting a fabric knuckle pattern thereon prior to drying and paper thereof1967704
US 3,473,576 AWeaving polyester fiber fabrics1969188
US 3,573,164 AFabrics with improved web transfer characteristics1971214
US 3,700,623 AReaction products of epihalohydrin and polymers of diallylamine and their use in paper1972594
US 3,772,076 AReaction products of epihalohydrin and polymers of diallylamine and their use in paper1973589
US 3,812,000 ASoft,absorbent,fibrous,sheet material formed by avoiding mechanical compression of the elastomer containing fiber furnished until the sheet is at least 80%dry1974186
US 3,821,068 ASoft,absorbent,fibrous,sheet material formed by avoiding mechanical compression of the fiber furnish until the sheet is at least 80% dry1974279
US 3,974,025 AAbsorbent paper having imprinted thereon a semi-twill, fabric knuckle pattern prior to final drying1976561
US 4,011,389 AGlycoside polyethers1977145
US 4,191,609 ASoft absorbent imprinted paper sheet and method of manufacture thereof1980656
US 4,208,459 ABonded, differentially creped, fibrous webs and method and apparatus for making same1980199
US 4,239,065 APapermachine clothing having a surface comprising a bilaterally staggered array of wicker-basket-like cavities1980408
US 4,300,981 ALayered paper having a soft and smooth velutinous surface, and method of making such paper1981576
US 4,476,323 ASurface-active quaternary ammonium compounds for treatment of textiles and cellulosic materials198457
US 4,497,716 AFabric softening composition198524