Method for improved recovery of metals
Abstract
Methodology for the extraction of metallic elements from solid and liquid metal-contaminated starting material such as mineral ores, recyclable wastes, contaminated soils, engraving solutions, metal finishing solutions, battery manufacturing solutions, toxic wastes such as dusts producing through steelmaking processes by effectuating preferably prolonged contacting of such starting material with liquor compositions to cause the underlying structure of the starting material to be broken down. The contaminated starting materials are more susceptible to metal separation because the released metallic element are readily solubilized in the contacting liquor. Compositions of the contacting liquor comprise caustic silicate solutions containing essentially saturating levels of silica. Once the plurality of metallic elements contained in the starting material have been solubilized, they tend to remain in solution, and then may be routinely extracted and removed using conventional extraction methodologies such as precipitation of insoluble salts, electrowinning, or electrodeposition.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 4.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for treating a liquid contaminated starting material having mineral elements and charged ions, said mineral elements and charged ions being solvated, chelated, or complexed in a structural arrangement, said method comprising the steps of: contacting said starting material with an aqueous caustic silica solution consisting of: an admixture of silica and at least one compound selected from the group consisting of sodium hydroxide, potassium hydroxide, and ammonium hydroxide; said aqueous caustic silica solution comprising from about 0.5% to about 5% w/w dissolved silica and about from 5
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (4 of 4 total)
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 5,549,811 A | Process for decontamination soils polluted with metals | 1996 | 10 |
Non-Patent Literature (2)
- Chemical Abstract Assession No 1975/142233; Abstract of Jp 49134599 A2, Dec. 25, 1974.
- Chemical Abstract Plus Assession No. 1975: 465188; Abstract of JP 50008371 A2, Jan. 28, 1975.*