Abstract
A Co-based alloy comprising 13-16 wt % Cr, 20-30 wt % Mo, 2.2-3.2 wt % Si, and balance Co, with a Cr:Si ratio of between about 4.5 and about 7.5, a Mo:Si ratio of between about 9 and about 15, wear resistance, and corrosion resistance in both oxidizing and reducing acids.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 9.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A Co-based alloy comprising: 13-16 wt % Cr, 20-30 wt % Mo,
- Claim 2Independent Claim
2-3.2 wt % Si, and 48-62 wt % Co.
- Claim 3Depends on #1
The alloy of claim 1 having corrosion resistance in reducing acid H 2 SO 4 characterized by less than about 50 mils/year (1.3 mm/year) thickness loss when tested according to ASTM specification G31-72 in a 10% solution at 102° C.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (9 of 9 total)
References Cited — Backward Prior Art (14)
Non-Patent Literature (5)
- ASTM Designation: E23-96, Standard Test Methods for Notched Bar Impact Testing of Metallic Materials, 1996.
- ASTM Designation: G 31-72, Standard Practice for Laboratory Immersion Corrosion Testing of Metals, 1972.
- ASTM Designation: G133-95, Standard Test Method for Linearly Reciprocating Ball-on-Flat Sliding Wear, 1995.
- Raghu, Damodaran, and Wu, James B. C., "Recent Developments in Wear- and Corrosion-Resistant Alloys for the Oil Industry", Materials Performance, 1997, pp. 27-36, vol. 36, No. 11.
- Schmidt, R. D. and Ferriss, D.P., "New Materials Resistant To Wear and Corrosion To 1000° C.", Wear, 1975, pp. 279-289, vol. 32, No. 3, Elsevier Sequoia S.A., Lausanne.