Patents
US 6,849,099 B2#3469939 Most CitedExpiredUnited States (USPTO)Utility

Polishing composition

23Forward Citations (#3469939 Global)
1.1/yrCitation Velocity (#5785215 Global)
3.28Citation PageRank (#6545824 Global)
12Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

There is provided a polishing composition that reduces erosion and is used in a final polishing step of a semiconductor device manufacturing process. The polishing composition contains colloidal silica, a periodic acid compound, ammonia, ammonium nitrate and water and its pH is 1.8 to 4.0.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 23.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A polishing composition used in a final polishing step of a manufacturing process of a semiconductor device, wherein the semiconductor device includes an insulation layer having a surface on which trenches are formed, and a conductive layer formed on the insulation layer, the polishing composition comprising: colloidal silica compounded in said polishing composition in a quantity larger than 50 g/liter and smaller than 160 g/liter; a periodic acid compound; ammonia; ammonium nitrate; and water, wherein the polishing composition has a pH that is in the range of 1.8 to 4.0.

  2. Claim 2Depends on #1

    The composition according to claim 1 , wherein the periodic acid compound is at least one compound selected from the group consisting of orthoperiodic acid, metaperiodic acid, dimesoperiodic acid, mesoperiodic acid, diorthoperiodic acid, ammonium periodate, potassium periodate

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗