Surface-treated rolling bearing and manufacturing method thereof
Abstract
In a rolling bearing put under a working circumstance in which water tends to intrude into lubricants, it has been known such a phenomenon that hydrogen ions formed by decomposition of the lubricants are adsorbed to raceway surfaces and accumulated as hydrogen atoms in highly strained sites (in the vicinity of the position for maximum shearing stress), to cause stress corrosion cracking type peeling. The present invention provides a rolling bearing in which an oxide layer of an iron/chromium oxide series is formed at a thickness of from 1 to 1000 nm to at least one of raceway surfaces of bearing rings or rolling contact surfaces of rolling elements and a manufacturing method thereof. The oxide layer can inhibit hydrogen formed by decomposition of water incorporated in the lubricants from intruding into the matrix of the bearing members, thereby preventing early peeling for the raceway surfaces of the bearing rings or the rolling contact surfaces of the rolling elements and, thus, greatly improving the rolling life. The oxide layer can be formed simply by merely tempering the bearing member and then applying a re-heating treatment in air at a temperature lower than the tempering tem
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 5.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A rolling bearing in which a plurality of rolling elements having a rolling contact surface are arranged between bearing rings comprising a fixed ring and a rotational ring having a raceway surface respectively, wherein at least one of the fixed ring, the rotational ring, and the rollings elements is made of a chromium containing alloy steel and at least one of the raceway surfaces of the bearing rings and the rolling contact surfaces of the rolling elements has an oxide layer comprising both iron oxide and chromium oxide, wherein the oxide layer has a thickness from 5 to 100 nm formed by re-h
- Claim 2Depends on #1
A rolling bearing as defined in claim 1 , wherein the surface hardness of the raceway surfaces of the bearing rings or the rolling contact surfaces of the rolling elements f
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (5 of 5 total)
References Cited — Backward Prior Art (15)
Non-Patent Literature (5)
- "Effects of Water and Oxygen During Rolling Contact Lubrication", Wear 12, pp. 331-342, 1968, P. Schatzberg, I.M. Felsen, no month data.
- "Handbook for Stainless Steel" by Nikkan Kogyo Shimbun Ltd. (First Ed.-Aug. 30, 1973) w/attached Translation of the Relevant Part, pp. 318-319 (4 pages).
- "The Surface-initiated and Subsurface-initiated Rolling Contact Fatigue", NSK Bearing Journal No. 636, pp. 1-10, 1977, Furumura, Shirota, Hirakawa, no month data available.
- Pretext for Japan Tribology Conference (Tokyo, May 1995), pp. 551-554.
- SAE Technical Paper: SAE 950944 (held on Feb. 27-Mar. 2, in 1995).