Glass funnel for a cathode ray tube and process for its production

10Forward Citations (#10796140 Global)
0.5/yrCitation Velocity (#17443047 Global)
1.64Citation PageRank (#19892253 Global)
26Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A glass funnel for a cathode ray tube, which has a substantially rectangular opened end at one end and a neck portion at the other end and which constitutes, together with a glass panel having a substantially rectangular face portion, a glass bulb to be used for a cathode ray tube, wherein the glass constituting the glass funnel contains, by molar percentage, at least 60% of SiO 2 and at least 7% of PbO; when the molar percentages of Na 2 O and K 2 O contained in said glass are represented by WNa and WK, respectively, 0.35≦WK/(WNa+WK)≦0.6; a compressive stress layer is formed by chemical tempering at least in the outer surface of a region containing a position where the tensile stress formed when the interior of the glass bulb is vacuumed to produce the cathode ray tube, becomes maximum; and either one or both of the outer surface of the chemically tempered region and the inner surface opposite to said outer surface, are colored by ion exchange coloration.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 26 · Forward citations: 10.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A glass funnel for a cathode ray tube, which has a substantially rectangular opened end at one end and a neck portion at the other end and which constitutes, together with a glass panel having a substantially rectangular face portion, a glass bulb to be used for a cathode ray tube, wherein the glass constituting the glass funnel contains, by molar percentage, at least 60% of SiO 2 and at least 7% of PbO; when the molar percentages of Na 2 O and K 2 O contained in said glass are represented by WNa and WK, respectively, 0.35≦WK/(WNa+WK)≦0.6; a compressive stress layer is formed by chemical temp