Golf ball compositions containing oxa esters
Abstract
A golf ball and process for forming a golf ball having at least one layer, where the layer is formed of a polymer blend comprising a thermoplastic component having a flexural modulus of about 60,000 psi or greater and at least one oxa ester, oxa acid, or a combination thereof. The thermoplastic component may be a high acid acid ionomer or a saponified ionomer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 38 · Forward citations: 0.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A golf ball having at least one layer, wherein the layer is formed of a polymer blend comprising: at least one ionomer comprising at least one α-olefin and at least one α, β-unsaturated carboxylic acid, wherein at least a portion of the acid groups are neutralized with at least one metal atom; and at least one oxa ester.
- Claim 2Depends on #1
The golf ball of claim 1 , wherein the ionomer comprises about 16 percent to about 35 percent by weight of the at least one α, β-unsaturated carboxylic acid.
- Claim 3Depends on #1
The golf ball of claim 1 , wherein the golf ball has an Atti compression of at least 50 and a coefficient of restitution of at least 0.7.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.