Method for treating slags or slag mixtures on an iron bath
Abstract
In a method for treating slags or slag mixtures having iron oxide contents of >5 wt.-%, in particular steelworks slags, in which the steel slags optionally mixed with other slags are charged onto a metal bath, a steel bath having a carbon content of <1.5 wt.-%, preferably <0.5 wt.-%, is used as the metal bath and the steel bath, after the charging of the steel slags, is carburized to above 2.0 wt.-% C, preferably >2.5 wt.-% C, by introducing carbon or carbon carriers.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 5.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for treating slags having iron oxide contents of greater than 5 percent by weight to form iron by reduction, comprising the steps of: charging the slags having iron oxide contents of greater than 5 percent by weight onto a steel bath having a carbon content of less than 1.5 percent by weight, and adding at least one of the group consisting of carbon and carbon carriers into said steel bath, whereby said steel bath is carburized to above 2.0 percent carbon by weight.
- Claim 2Depends on #1
A method according to claim 1 , wherein said slags are charged onto a steel bath having a carbon content of less than 0.5 percent carbon by weight.
- Claim 3Depends on #1
A method according to claim 1 , wherein said steel bath is carburized to above 2.5 percent carbon by weight.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗