Method for brazing aluminum alloy-assembled articles within a short period of time and a filler alloy usable at low temperature
Abstract
A method for brazing aluminum alloy-assembled articles with a filler alloy having a liquidus temperature of 540° C. or lower and a difference of temperature between the liquidus temperature and the solidus temperature being 100° C. or lower, wherein the highest temperature reached in the assembled article at the time of heating for brazing being set 40° C. or more higher than the liquidus temperature but 585° C. or lower. An aluminum alloy-filler alloy usable at low temperature for brazing, which comprises Si in an amount of 4.0 wt % to 8.0 wt %, Zn in an amount of 7.0 wt % to 20.0 wt % and Cu in an amount of 10.0 wt % to 35.0 wt %, with the balance being made of aluminum.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 6.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for brazing aluminum alloy-assembled articles within a short period of time, wherein an Al alloy having a liquidus temperature of 540° C. or lower and a difference of temperature between the liquidus and the solidus temperature being 100° C. or lower and containing approximately 6.0 wt % of Si, 25.0 wt % of Cu, and 5.0 wt % of Zn is used as the filler alloy, wherein the highest temperature reached in the assembled articles at the time of heating for brazing is set 40° C. or more higher than the liquidus temperature but 585° C. or lower.
- Claim 2Independent Claim
A method for brazing aluminum alloy-assembled articles within a short period of time, which comprises brazing aluminum alloy-assembled articles with a filler alloy of Al—Si—Cu—Zn series having a liquidus temperature of 540° C. or lower and a difference of temperature between the liquidus and the solidus temperature being
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗