Patents
US 6,835,660 B2#22450390 Most CitedExpiredUnited States (USPTO)Utility

Method of manufacturing semiconductor device having metal alloy interconnection that has excellent EM lifetime

5Forward Citations (#22450390 Global)
0.2/yrCitation Velocity (#31001221 Global)
1.11Citation PageRank (#36297068 Global)
3Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

In a method of manufacturing a semiconductor device of the invention, a substrate insulating film 102 is formed on a semiconductor substrate 100, a barrier layer 104 is formed on the substrate insulating film, an Al-Cu interconnection layer 106 is formed on the barrier layer by sputtering under a condition that the nitrogen concentration in the atmosphere in the sputtering deposition chamber is higher than 12 ppm but lower than 1000 ppm, and then an anti-reflective film 108 is formed on the Al-Cu interconnection layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 5.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a semiconductor device, comprising; depositing an Al—Cu interconnection layer with a nitrogen concentration in an atmosphere in a sputtering deposition chamber made to be higher than 12 ppm but lower than 1000 ppm.

  2. Claim 2Depends on #1

    The method of manufacturing a semiconductor device according to claim 1 , wherein the nitrogen concentration in the atmosphere in the sputtering deposition chamber is controlled by introducing nitrogen-containing argon gas into the deposition chamber.

  3. Claim 3Depends on #2

    The method of manufacturing a semiconductor device according to claim 2 , wherein in the case that the nitrogen concentration is made to be less than 200 ppm, the nitrogen concentration is controlled by introducing into the deposition chamber argon gas to which has been added 0.1% of nitrogen as a partial press

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗