US 6,835,633 B2#3514382 Most CitedExpiredUnited States (USPTO)Utility

SOI wafers with 30-100 Å buried oxide (BOX) created by wafer bonding using 30-100 Å thin oxide as bonding layer

23Forward Citations (#3514382 Global)
1.1/yrCitation Velocity (#6109540 Global)
2.54Citation PageRank (#9923669 Global)
3Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of fabricating a SOI wafer having a gate-quality, thin buried oxide region is provided. The wafer is fabricating by forming a substantially uniform thermal oxide on a surface of a Si-containing layer of a SOI substrate which includes a buried oxide region positioned between the Si-containing layer and a Si-containing substrate layer. Next, a cleaning process is employed to form a hydrophilic surface on the thermal oxide. A carrier wafer having a hydrophilic surface is provided and positioned near the substrate such that the hydrophilic surfaces adjoin each other. Room temperature bonding is then employed to bond the carrier wafer to the substrate. An annealing step is performed and thereafter, the Si-containing substrate of the silicon-on-insulator substrate and the buried oxide region are selectively removed to expose the Si-containing layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 23.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A bonded structure comprising: a silicon-on-insulator substrate having a substantially uniform thermal oxide film present atop a Si-containing layer, said thermal oxide having a hydrophilic surface region; and a carrier wafer comprising a Si-containing semiconductor selected from the group consisting of Si, SiGe, SiGeC, Si/Si, Si/SiC and Si/SiGeC, and having a hydrophilic Si-containing semiconductor surface, wherein said hydrophilic surfaces are bonded together.

  2. Claim 2Depends on #1

    The bonded structure of claim 1 wherein said thermal oxide film has a thickness of from about 30 to about 100 Å.

  3. Claim 3Depends on #1

    The bonded structure of claim 1 wherein said silicon-on-insulator substrate comprising a buried oxide region sandwiched between a Si-containing layer and a Si-containing substrate.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗