Method and depositing a layer

2Forward Citations (#36371571 Global)
0.1/yrCitation Velocity (#46911952 Global)
1.18Citation PageRank (#33170531 Global)
19Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

This invention relates to a method of depositing a layer on an exposed surface of an insulating layer of material. The method includes treating the exposed surface with hydrogen or a gaseous source of hydrogen in the presence of a plasma, prior to or during deposition of a metallic layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of depositing a metallic layer on an exposed surface of previously deposited insulating layer on a substrate, said method comprising: treating the exposed surface with hydrogen or a gaseous source of hydrogen in the presence of a plasma; and depositing the metallic layer over the exposed surface, wherein the hydrogen treatment occurs prior to or during the deposition of the metallic layer, and wherein a duration and plasma power of the hydrogen treatment are sufficient to improve the crystal orientation of the deposited metallic layer such that the x-ray diffraction peak half width on

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (19)

PatentTitleYearCitations
US 5,242,860 AMethod for the formation of tin barrier layer with preferential (111) crystallographic orientation199390
US 5,278,448 ASemiconductor device and method of fabricating the same199422
JP H07142412 ADeposition of thin metal film in semiconductor device—7
US 5,462,890 AMethod for making a tungsten plug of a semiconductor device199519
US 5,523,259 AMethod of forming metal layers formed as a composite of sub-layers using Ti texture control layer199649
JP H08274076 AManufacture of semiconductor device—6
US 5,591,663 AMethod of manufacturing ferroelectric capacitor with a hydrogen heat treatment199729
JP H09246212 AFormation of barrier layer and semiconductor device with barrier layer formed thereby—11
US 5,795,823 ASelf aligned via dual damascene1998114
US 5,843,843 AMethod for forming a wiring layer a semiconductor device199880
US 5,851,917 AMethod for manufacturing a multi-layer wiring structure of a semiconductor device199821
JP H1140518 AFilm formation of cvd-titanium film—11
US 5,899,720 AProcess of fabricating salicide structure from high-purity reproducible cobalt layer without sacrifice of leakage current and breakdown voltage of P-N junction199971
US 6,001,736 AMethod of manufacturing semiconductor device and an apparatus for manufacturing the same199936
US 6,025,762 ADelay line incorporating a surface acoustic wave ladder filter and method of providing same200013
US 6,077,571 AConformal pure and doped aluminum coatings and a methodology and apparatus for their preparation200049
US 6,143,128 AApparatus for preparing and metallizing high aspect ratio silicon semiconductor device contacts to reduce the resistivity thereof200050
US 6,204,192 B1Plasma cleaning process for openings formed in at least one low dielectric constant insulation layer over copper metallization in integrated circuit structures2001145

Non-Patent Literature (3)

  • C.R. Aita, "Basal orientation aluminum nitride grown . . . ", J. Appl. Phys. 53(3), Mar. 1982, pp. 1807-1808.
  • Hiroshi Okano et al., "Preparation of c-Axis Oriented AIN Thin Films by Low-Temperature Reactive Sputtering", Jpn. J. Appl. Phys. Vol. 31 (1992), Pt. 1. No. 10, pp. 3446-3451.
  • Hwan-Chul Lee et al., "Effects of sputtering pressure and nitrogen concentration on the preferred orientation of AIN thin films," Journal of Materials Science: Materials in Electronics (1994) 221-225.