Nickel silicide—silicon nitride adhesion through surface passivation
Abstract
A process for forming nickel silicide and silicon nitride structure in a semiconductor integrated circuit device is described. Good adhesion between the nickel silicide and the silicon nitride is accomplished by passivating the nickel suicide surface with nitrogen. The passivation may be performed by treating the nickel silicide surface with plasma activated nitrogen species. An alternative passivation method is to cover the nickel silicide with a film of metal nitride and heat the substrate to about 500° C. Another alternative method is to sputter deposit silicon nitride on top of nickel silicide.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 5.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process of forming a semiconductor device, comprising a. providing a substrate having a top surface, at least a portion of the top surface including a region of a silicide material; b. subjecting the top surface that includes the region of the silicide material to an environment that contains activated species of nitrogen and that is substantially devoid of silicon to prevent the formation of a silicon-rich layer and to form a nitrogen passivated silicide surface; and c. forming on the nitrogen passivated silicide surface a dielectric layer that includes silicon.
- Claim 2Depends on #1
The process of claim 1 , wherein the silicide material includes nickel silicide.
- Claim 3Depends on #2
The process in claim 2 , further comprising forming the nickel silicide region with a self-aligned process.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (5 of 5 total)
References Cited — Backward Prior Art (5)
Non-Patent Literature (1)
- Pending U.S. application No. 10/288,717 filed Nov. 6, 2002, "Method for Reducing Contamination, Copper Reduction, and Depositing a Dielectric Layer on a Semiconductor Device", Tessmer et al.