US 6,830,594 B2#21433854 Most CitedExpiredUnited States (USPTO)Utility

Process for producing an electric double layer capacitor and positive electrode for an electric double layer capacitor

5Forward Citations (#21433854 Global)
0.2/yrCitation Velocity (#30837713 Global)
1.39Citation PageRank (#25845577 Global)
7Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A process for producing an electric double layer capacitor, which comprises a step of preparing a positive electrode and a negative electrode, each being a carbonaceous electrode containing as the main component a carbon material having a specific surface area of from 100 to 2,500 m<2>/g, a step of forming an element comprising the positive electrode and the negative electrode and a separator having a thickness of at most 60 mum interposed therebetween, and a step of impregnating the element with a non-aqueous electrolyte, wherein the copper content in the positive electrode before being impregnated with the non-aqueous electrolyte is at most 1 ppm.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 5.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for producing an electric double layer capacitor, which comprises a step of preparing a positive electrode and a negative electrode, each being a carbonaceous electrode containing as the main component a carbon material having a specific surface area of from 100 to 2,500 m 2 /g, a step of forming an element comprising the positive electrode and the negative electrode and a separator having a thickness of at most 60 μm interposed therebetween, and a step of impregnating the element with a non-aqueous electrolyte, wherein the copper content in the positive electrode before being impreg

  2. Claim 2Depends on #1

    The process for producing an electric double layer capacitor according to claim 1 , wherein the copper content in the carbon material is at most 1 ppm.

  3. Claim 3Independent Claim

    The pr

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗