Method of forming a device isolation trench in an integrated circuit device

18Forward Citations (#4905757 Global)
0.8/yrCitation Velocity (#8940899 Global)
3.17Citation PageRank (#6932481 Global)
8Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method of forming a trench isolation in a semiconductor substrate is described, which comprises the steps of forming a trench on the substrate, forming a diffusion barrier insulating layer, forming a thermal oxide layer both sidewall and bottom of the trench contacted with the diffusion barrier insulating layer, forming a nitride liner, and forming trench isolation material to fill the trench. A multi-structure of the barrier layer and the thermal oxide layer is provided between the nitride liner and the trench, resulting in minimization of transistor characteristic deterioration. A thin thermal oxide layer is formed to achieve improved trench etching profile.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 18.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of forming an isolation trench including a nitride liner in a semiconductor substrate, comprising: etching the substrate to form a trench therein; forming a conformal material layer on sidewall and bottom of the trench, wherein the conformal material layer comprises a material selected from the group consisting of high temperature oxide (HTO), aluminum trioxide (Al 2 O 3 ), and tantalum pentaoxide (Ta 2 O 5 ); growing a thermal oxide layer between the conformal material layer and the substrate; forming the nitride liner on the material layer; and filling the trench with a trench isola

  2. Claim 2Depends on #1

    The method as claimed in claim 1 , wherein the conformal material layer is formed to a thickness of 50 Å-400 Å, and the thermal oxide layer is formed to a thickness of 20 Å-150 Å