Embedding resin and wiring substrate using the same
Abstract
In an embedding resin for embedding electronic parts, after a substrate in which a copper layer is formed on a cured product of the embedding resin is subjected to a pressure cooker test, the copper layer has a peeling strength of at least 588 N/m (0.6 kg/cm), wherein the conditions of the pressure cooker test are 121° C., 100% by mass humidity, 2.1 atm and 168 hours, and the measurement method of the peeling strength is according to JIS C 5012, and the width of the copper layer is 10 mm.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 46.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
An embedding resin for embedding electronic parts, wherein after a substrate in which a copper layer is formed on a cured product of the embedding resin is subjected to a pressure cooker test, the copper layer has a peeling strength of at least 588 N/m (0.6 kg/cm), wherein the conditions of the pressure cooker test are 121° C., 100% by mass humidity, 2.1 atm and 168 hours, and the measurement method of the peeling strength is according to JIS C 5012, and the width of the copper layer is 10 mm.
- Claim 2Independent Claim
An embedding resin for embedding electronic parts, wherein after a substrate in which a copper layer is formed on a cured product of the embedding resin is subjected to a pressure cooker test, the copper layer has a peeling strength of at least 600 N/n (0.61 kg/cm), wherein the conditions of the pressure
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 46 total)
References Cited — Backward Prior Art (10)
Non-Patent Literature (3)
- English Abstract JP 11126978, May 11, 1999.
- English Abstract JP 2000124352, Apr. 28, 2000.
- English Abstract JP 9046046, Feb. 14, 1997.