US 6,814,820 B2#4619919 Most CitedExpiredUnited States (USPTO)Utility

Heat treatment of titanium-alloy article having martensitic structure

19Forward Citations (#4619919 Global)
0.9/yrCitation Velocity (#8393493 Global)
2.69Citation PageRank (#9051823 Global)
10Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An article is formed of an alpha-beta titanium-base alloy, preferably an alloy having more than about 3.5 weight percent molybdenum. An example of such an article is a gas turbine compressor blade having a nominal composition, in weight percent, of about 4 percent aluminum, about 4 percent molybdenum, about 2 percent tin, about 0.5 percent silicon, balance titanium and impurities. The article is processed to form a martensitic structure therein. The processing, which typically involves forging or weld repairing, includes the steps of first heating the article to a first-heating temperature of greater than about 1600° F., and thereafter first cooling the article to a temperature of less than about 800° F. The article is thereafter second heated to a second-heating temperature of from about 1275° F. to about 1375° F. for a time of from about 1 to about 7 hours, and thereafter second cooled to a temperature of less than about 800° F. at a second cooling rate that does not exceed about 15° F. per second.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 19.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for heat treating an article, comprising the steps of: providing an article having a nominal composition, in weight percent, of about 4 percent aluminum, about 4 percent molybdenum, about 2 percent tin, about 0.5 percent silicon, balance titanium and impurities; processing the article to form a martensitic structure therein, the step of processing including the steps of first heating the article to a first-heating temperature of greater than about 1600° F. and in the alpha-plus-beta region of a phase diagram of the article, and thereafter first cooling the article to a temperature of

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • ASM Handbook, 10<th >Edition, vol. 2, "Wrought Titanium and Titanium Alloys: Titanium Alloys", ASM International, 1992.*
  • ASM Handbook, 10th Ed., vol. 2, Section on Titanium alloys, 1992.*
  • ASM Handbook, 10th Edition, vol. 2, "Titanium and Titanium Alloy Castings: Weld Repair", ASM International, 1992.*
  • ASM Handbook, 10th Edition, vol. 2, "Wrought Titanium and Titanium Alloys: Properties", ASM International, 1992.*
  • ASM Handbook, 10th Edition, vol. 2, "Wrought Titanium and Titanium Alloys: Titanium Alloys", ASM International, 1992.*