Articles formed from propylene diene copolymers
Abstract
The co-polymerization reaction of one or more olefin monomers, such as propylene, with alpha,omega-diene units and the resulting copolymers are provided. More specifically, the copolymer may have from 90 to 99.999 weight percent of olefins and from 0.001 to 2.000 weight percent of alpha,omega-dienes. The copolymer may have a weight average molecular weight in the range from 50,000 to 2,000,000, a crystallization temperature in the range from 115° C. to 135° C. and a melt flow rate in the range from 0.1 dg/min to 100 dg/min. These copolymers may be employed in a wide variety of applications, the articles of which include, for example, films, fibers, such as spunbonded and meltblown fibers, fabrics, such as nonwoven fabrics, and molded articles. The copolymer may further include at least two crystalline populations. Desirably, the melting point range of one of the crystalline populations is distinguishable from the melting point range of another crystalline population by a temperature range of from 1° C. to 8° C. More desirably, one of the crystalline populations has a melting point in the range from 152° C. to 158° C. and another crystalline population has a melting point in the ran
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 10.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
An article comprising copolymer comprising from 90 to 99.999 weight percent of olefin units, from 0.001 to 2.000 weight percent of α,ω-diene units, wherein the copolymer has a weight average molecular weight in the range from 50,000 to 2,000,000, a melt flow rate in the range from 0.1 dg/min to 100 dg/min, and the copolymer has a first melting point in a first melting point range and a second melting point in a second melting point range and wherein the first melting point range is distinguishable from the second melting point range by a temperature range of from 1° C. to 8° C.
- Claim 2Depends on #1
The article of claim 1 wherein the weight percent of α,ω-diene units present in the copolymer is from 0.005 to 1.5.
- Claim 3Depends on #1
The article of claim 1 wherein the weight percent of α,ω-diene units present in the copolymer is from 0.005 to
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (10 of 10 total)
References Cited — Backward Prior Art (50)
Non-Patent Literature (5)
- Japanese Patent JP 05 194659 A2 (Aug. 3, 1993) Derwent Abstract, "Olefin copolymers with high melt tension and manufacture thereof"-Shinozaki et al.,-Mitsui Petrochemical, Japan.
- Japanese Patent JP 06 093041 A2 (Apr. 5, 1994) Derwent Abstract,, "Manufacture of reactive propylene random copolymers free from boiling xylene-insoluble components"-Goto et al.-Mitsubishi Petrochemical, Japan.
- Japanese Patent JP 06 093042 A2 (Apr. 5, 1994) Derwent Abstract, "Catalysts and manufacture of propylene random copolymers"-Futamura et al.,-Mitsubishi Petrochemical, Japan.
- Japanese Patent JP 07 133387 A2 (May 23, 1995) Derwent Abstract, "Propylene polymer compositions with balanced rigidity and impact resistance"-Sugimoto et al.,-Mitsui Toatsu Chemicals, Japan.
- Japanese Patent JP 07 138424 A2 (May 30, 1995) Derwent Abstract, "Propylene polymer compositions with balanced rigidity"-Sugimoto et al.,-Mitsui Toatsu Chemicals, Japan.