Abstract
The present invention provides non-heat cleaned glass fiber fabrics comprising resin compatible coatings that offer higher tensile strengths than corresponding fabrics that have been heat cleaned and silane finished. These fabrics can be used in a wide variety of applications, such as reinforcements for composites such as printed circuit boards. In one nonlimiting embodiment, the invention provides a non-heat cleaned fabric comprising a plurality of fiber strands in a warp direction and a fill direction, each fiber strand comprising a plurality of E-glass fiber, and having a resin compatible coating composition on at least a portion of a surface of at least one fiber strand, wherein the fabric has a tensile strength of at least 267 Newtons when measured in the warp direction or fill direction. Although not required, the fabric also has a tensile strength of at least 1.5 times that of a corresponding fabric that is heat cleaned by heating the corresponding fabric to a temperature of at least 380° C. for at least 60 hours and silane finished when measured in the warp direction or fill direction.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 0.
Claims (19)
- Claim 1Independent Claim
A non-heat cleaned fabric comprising a plurality of fiber strands in a warp direction and a fill direction, each fiber strand comprising a plurality of E-glass fiber, and having a resin compatible coating composition on at least a portion of a surface of at least one fiber strand, wherein the fabric has a tensile strength of at least 267 Newtons when measured in the warp direction or fill direction.
- Claim 2Depends on #1
A fabric according to claim 1 , wherein the fabric has a tensile strength of 445 Newtons.
- Claim 3Depends on #2
A fabric according to claim 2 , wherein the fabric has a tensile strength of 667 Newtons.
- Claim 4Depends on #3
A fabric according to claim 3 , wherein the fabric has a tensile strength of 1334 Newtons.
- Claim 5Depends on #1
A fabric according to claim 1 , wherein the fabric has a tensile strength of at least 1.5 times that of a corresponding fabric that is heat cleaned by heating the corresponding fabric to a temperature of at least 380° C. for at least 60 hours and silane finished when measured in the warp direction or fill direction.
- Claim 6Depends on #5
A fabric according to claim 5 , wherein the fabric has a tensile strength of at least 2 times that of a corresponding fabric that is heat cleaned by heating the corresponding fabric to a temperature of at least 380° C. for at least 60 hours and silane finished when measured in the warp direction or fill direction.
- Claim 7Depends on #6
A fabric according to claim 6 , wherein the fabric has a tensile strength of at least 3 times that of a corresponding fabric that is heat cleaned by heating the corresponding fabric to a temperature of at least 380° C. for at least 60 hours and silane finished when measured in the warp direction or fill direction.
- Claim 8Depends on #1
A fabric according to claim 1 , wherein the fabric is selected from 7628, 2116 and 1080 style fabrics.
- Claim 9Depends on #8
A fabric according to claim 8 , wherein the fabric is a 7628 style fabric and the tensile strength is at least 667 Newtons.
- Claim 10Depends on #9
A fabric according to claim 9 , wherein the fabric has a tensile strength of at least 890 Newtons.
- Claim 11Depends on #10
A fabric according to claim 10 , wherein the fabric has a tensile strength of at least 1334 Newtons.
- Claim 12Depends on #8
A fabric according to claim 8 , wherein the fabric is a 2116 style fabric and has a tensile strength of at least 445 Newtons.
- Claim 13Depends on #12
A fabric according to claim 12 , wherein the fabric has a tensile strength of at least 667 Newtons.
- Claim 14Depends on #8
A fabric according to claim 8 , wherein the fabric is a 1080 style fabric and has a tensile strength of at least 334 Newtons.
- Claim 15Depends on #14
A fabric according to claim 14 , wherein the fabric has a tensile strength of at least 400 Newtons.
- Claim 16Depends on #8
A fabric according to claim 8 , wherein the fabric has a tensile strength of at least 1.5 times that of a corresponding fabric that is heat cleaned by heating the corresponding fabric to a temperature of at least 380° C. for at least 60 hours and silane finished when measured in the warp direction or fill direction.
- Claim 17Depends on #16
A fabric according to claim 16 , wherein the fabric has a tensile strength of at least 2 times that of a corresponding fabric that is heat cleaned by heating the corresponding fabric to a temperature of at least 380° C. for at least 60 hours and silane finished when measured in the warp direction or fill direction.
- Claim 18Depends on #17
A fabric according to claim 17 , wherein the fabric has a tensile strength of at least 3 times that of a corresponding fabric that is heat cleaned by heating the corresponding fabric to a temperature of at least 380° C. for at least 60 hours and silane finished when measured in the warp direction or fill direction.
- Claim 19Depends on #8
A fabric according to claim 8 , wherein the fabric is a 7628 styl
Technical Overview & Description
RELATED APPLICATIONS This application is a continuing application of U.S. patent application Ser. No. 09/527,034 of Novich et al. entitled “Impregnated Glass Fiber Strands and Products Including the Same”, filed Mar. 16, 2000, which claims the benefit of U.S. Provisional Application Nos. 60/146,605 filed Jul. 30, 1999; No. 60/146,862 filed Aug. 3, 1999; and No. 60/183,562 filed Feb. 18, 2000. This application also claims the benefit of U.S. Provisional Application No. 60/233,460 filed Sep. 18, 2000. This invention relates generally to non-heat cleaned fabric comprising resin compatible yarn and, in particular to the tensile strength of such fabrics. In thermosetting molding operations, good “wet-through” (penetration of a polymeric matrix material through the mat or fabric) and “wet-out” (penetration of a polymeric matrix material through the individual bundles or strands of fibers in the mat or fabric) properties are desirable. In contrast, good dispersion properties (i.e., good distribution properties of fibers within a thermoplastic material) are of predominant concern in typical thermoplastic molding operations. In the case of composites or laminates formed from fiber strands woven into fabrics, in addition to providing good wet-through and good wet-out properties of the strands, it is desirable that the coating on the surfaces of the fibers strands protect the fibers from abrasion during processing, provide for good weavability, particularly on air-jet looms and be compatible with the polymeric matrix material into which the fiber strands are incorporated. However, many sizing components are not compatible with the polymeric matrix materials and can adversely affect adhesion between the glass fibers and the polymeric matrix material. For example, starch, which is a commonly used sizing component for textile fibers, is generally not compatible with polymeric matrix material. As a result, these incompatible materials must b
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (6)
| Patent | Title | Year | Citations |
|---|