Composition for shielding radioactivity
Abstract
A urethane based polymer composition is provided that exhibits superior shielding properties during and after exposure to high level radiation. The composite is formed by mixing a liquid isocyanate monomer, preferably 4,4′-diisocyanate monomer with a liquid phenolic resin, preferably phenol formaldehyde resin, and a phosphate ester flame retardant. An optional pyridine catalyst may be added to shorten the cure time. The resulting composition cures at room temperature and can be utilized in several manners, including spraying or pouring the composition prior to curing over radioactive material to prevent leakage of radiation. The uncured composite can be sprayed on the walls of a room or container to prevent leakage of radiation and can also be used to contain radiation prior to demolition. The uncured composite can also be molded into bricks or panels for use in construction. In a preferred embodiment, the polymer composition further incorporates radioactive waste, namely depleted uranium oxide, and can be used in conjunction with specially designed containers for storing radioactive material. The resulting polymer/waste composition cures at room temperature and does not deteriorate or suffer structural damage when exposed to higher levels of gamma radiation, nor do the mechanical or chemical properties undergo any detectable change. The composition is resistant to biodegradation and combustion, and does not creep or shrink during thermal cycling.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 1.
Claims (13)
- Claim 1Independent Claim
A polymer composition for radiation shielding comprising: about 1.2 to 15% at least one isocyanate monomer; about 1.0 to 14% at least one phenolic resin; about 0.2 to 1.0% at least one flame retardant compound; and about 80 to 96% depleted uranium, wherein the isocyanate monomer, phenolic resin, and depleted uranium of the composition are combined to form a homogeneous mixture prior to curing of the composition.
- Claim 2Depends on #1
The polymer composition of claim 1 wherein the isocyanate monomer is an aromatic isocyanate.
- Claim 3Depends on #1
The polymer composition of claim 1 wherein the phenolic resin is produced by the polycondensation of a phenol compound with formaldehyde.
- Claim 4Independent Claim
The polymer composition of claim I wherein the depleted uranium is selected from the group consisting of UO 3 , UO 2 , U 3 O 8 , and mixtures thereof.
- Claim 5Depends on #1
The polymer composition of claim 1 further comprising a catalyst.
- Claim 6Independent Claim
A polymer composition for radiation shielding comprising: about 1.2 to 15% at least one aromatic isocyanate monomer; about 1.0 to 14% at least one phenolic resin, the phenolic resin being produced by the polycondensation of a phenol compound with formaldehyde; about 80 to 96% depleted uranium selected from the group consisting of UO 3 , UO 2 , U 3 O 8 and mixtures thereof; about 0.2 to 1.0% at least one halogenated phosphate ester flame retardant and about 0 to 1.0% at least one catalyst; wherein the isocyanate monomer, phenolic resin, and depleted uranium of the composition are combined to form a homogeneous mixture prior to curing of the composition.
- Claim 7Depends on #6
The polymer composition of claim 6 wherein the aromatic isocyanate monomer is diphenylmethane 4,4′-diisocyanate.
- Claim 8Depends on #6
The polymer composition of claim 6 wherein the phenolic resin is produced by the polycondensation of phenol with formaldehyde.
- Claim 9Depends on #6
The polymer composition of claim 6 wherein the catalyst is phenylpropyl pyridine.
- Claim 10Depends on #6
The polymer composition of claim 6 wherein the halogenated phosphate ester flame retardant is Firemaster 836™.
- Claim 11Independent Claim
A polymer composition for radiation shielding comprising: about 2.4% diphenylmethane 4,4′-diisocyanate; about 3.6% phenolic resin, the phenolic resin being produced by the polycondensation of phenol with formaldehyde; about 0.6% halogenated phosphate ester; and about 93.4% depleted uranium selected from the group consisting of UO 3 , UO 2 , U 3 O 8 and mixtures thereof; wherein the diphenylmethane 4,4′-diisocyanate, phenolic resin and depleted uranium of the composition are combined to form a homogeneous mixture prior to curing of the composition.
- Claim 12Independent Claim
A polymer composition for radiation shielding comprising: about 2.4% diphenylmethane 4,4′-diisocyanate; about 3.6% phenolic resin, the phenolic resin being produced by the polycondensation of phenol with formaldehyde; about 93.25% depleted uranium selected from the group consisting of UO 3 , UO 2 , U 3 O 8 and mixtures thereof; about 0.6% halogenated phospate ester and about 0.15% phenylpropyl pyridine; wherein the diphenylmethane 4,4′-diisocyanate, phenolic resin, depleted uranium and phenypropyl pyridine of the composition are combined to form a homogeneous mixture prior to curing of the composition.
- Claim 13Independent Claim
The process of making a polymer composition comprising: mixing about 1.2 to 15% at least one isocyanate monomer; about 1.0 to 14% phenolic resin; about 0.2 to 1.0% flame retardant compound; and about 80 to 96% depleted uranium, until a homogeneous mixture is formed; and allowing the homogeneous mixture to cur
Technical Overview & Description
This application claims the benefit of U.S. Provisional Application Ser. No. 60/206,853 filed May 24, 2000; U.S. Provisional Application Ser. No. 60/206,888 filed May 24, 2000; and U.S. Provisional Application Ser. No. 60/210,393 filed Jun. 9, 2000. FIELD OF THE INVENTION The present invention relates generally to a composition and method for shielding radioactivity and, more particularly, to a modified urethane/phenolic resin polymer composition shielding material capable of encapsulating and stabilizing nuclear waste within a polymeric matrix, and methods for using the polymer composition. Nuclear waste generated by the nuclear energy industry must be immobilized for safety and environmental reasons. The polymer composition of the present invention effectively immobilizes nuclear waste in the polymeric matrices safely and in a cost-effective manner. Further, when depleted uranium is the waste incorporated in the polymeric matrix, the polymer composition is a highly effective radiation shielding material that can be stored or utilized for secondary applications. BACKGROUND OF THE INVENTION The tremendous growth in the nuclear energy industry demands the need for safe, cost effective immobilization of wastes generated. Nuclear power generation is dependent on enriched uranium-235 fuel. Given the natural abundance of the U-235 isotope is 0.7%, large quantities of uranium-238 isotope, known as depleted uranium, remain after processing. As there is very little demand for this isotope, U-238 is stockpiled. One Department of Energy storage site in Paducah, Kentucky has 700,000 tons of depleted uranium in storage. Depleted uranium is a very low radiation source, but is very toxic and environmentally hazardous. Further, transportation to other storage sites is not feasible for economic and safety reasons. In addition, the depleted uranium waste, which is stored underground, is often kept under heavy mineral oil to prevent atmos
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 12,148,541 B2 | Ventilated cask for nuclear waste storage | 2024 | 0 |
References Cited — Backward Prior Art (14)
| Patent | Title | Year | Citations |
|---|