Patents
US 6,803,028 B2#15586477 Most CitedExpiredUnited States (USPTO)Utility

Method of making stoichiometric lithium niobate

7Forward Citations (#15586477 Global)
0.3/yrCitation Velocity (#24923157 Global)
1.62Citation PageRank (#20209146 Global)
12Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Methods of manufacturing stoichiometric lithium niobate elements are provided. The method involves heating lithium niobate substrates in the presence of a monolithic sintered source of lithium and/or niobium. The method is useful for producing lithium niobate optical elements such as waveguides, switches and modulators.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 7.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of changing the stoichiometry of a lithium niobate substrate comprising: mixing powders containing lithium and niobium; sintering the powders to provide a monolithic solid; and placing the monolithic solid proximate to the lithium niobate substrate and heating the monolithic solid and substrate to a temperature between 800° C. and 1200° C. for a period of time sufficient to change the stoichiometry in a portion of the substrate.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the powders are selected from the group consisting of lithium oxide, lithium carbonate, niobium oxide, niobium carbonate, lithium nitrate and mixtures thereof.

  3. Claim 3Depends on #2

    The method of claim 2 , wherein the powders are sintered at a temperature between 500° C. and 1200° C. for less than five hours.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗