Soft magnetic film having high saturation magnetic flux density, thin film magnetic head using the same, and methods of producing the soft magnetic film and the thin film magnetic head
Abstract
A lower pole layer and/or an upper pole layer is formed by plating a NiFe alloy having a Fe composition ratio of 76% by mass to 90% by mass, or having an average crystal grain diameter of 130 Å to 175 Å and a Fe composition ratio of 70% by mass to 90% by mass. As a result, the saturation magnetic flux density can be increased to 1.9 T or more, and a thin film magnetic head excellent for a higher recording density can be manufactured.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 19.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A soft magnetic film having a composition represented by the formula Ni 1-X Fe X wherein the Fe composition ratio X is 76% by mass to 90% by mass, wherein an average crystal grain diameter is 150 Å to 175 Å.
- Claim 2Depends on #1
A soft magnetic film according to claim 1 , wherein the saturation magnetic flux density Bs is 1.95 T or more.
- Claim 3Depends on #1
A soft magnetic film according to claim 1 , wherein coercive force Hc is 553 (A/m) or less.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗