Patents
US 6,800,670 B2#1066649 Most CitedExpiredUnited States (USPTO)Utility

Crosslinking of polyethylene for low wear using radiation and thermal treatments

47Forward Citations (#1066649 Global)
2.1/yrCitation Velocity (#1795239 Global)
3.08Citation PageRank (#7269025 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present invention discloses methods for enhancing the wear-resistance of polymers, the resulting polymers, and in vivo implants made from such polymers. One aspect of this invention presents a method whereby a polymer is irradiated, preferably with gamma radiation, then thermally treated, such as by remelting of annealing. The resulting polymeric composition preferably has its most oxidized surface layer removed. Another aspect of the invention presents a general method for optimizing the wear resistance and desirable physical and/or chemical properties of a polymer by crosslinking and thermally treating it. The resulting polymeric compositions is wear-resistant and may be fabricated into an in vivo implant.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 47.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    An implantable bearing component made by the process comprising the steps of: (a) crosslinking, by irradiation, a preformed polymer in its solid state; (b) remelting the crosslinked polymer; and (c) fashioning the implantable bearing component from the crosslinked and remelted polymer, wherein the polymer is selected from the group consisting of: polyester, poly(methylmethacrylate), nylon, polycarbonates, and polyhydrocarbons.

  2. Claim 2Depends on #1

    The implantable bearing component of claim 1 , wherein the polymer is crosslinked by gamma radiation at a dose of from about 1 to about 100 Mrad.

  3. Claim 3Depends on #2

    The implantable bearing component of claim 2 , wherein the gamma radiation dose is from about 4.5 to about 25 Mrad.