Patents
US 6,800,243 B2#5051414 Most CitedExpiredUnited States (USPTO)Utility

Titanium alloy and method for heat treatment of large-sized semifinished materials of said alloy

18Forward Citations (#5051414 Global)
0.8/yrCitation Velocity (#8987368 Global)
2.02Citation PageRank (#14287465 Global)
6Prior Art Cited
3Claims (3 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The inventive titanium alloy comprises, expressed in mass %: aluminium 4.0-6.0; vanadium 4.5-5.0; molybdenum 4.5-5.0; chromium 2.0-3.6; ferrum 0.2-0.5; the rest being titanium. An equivalent molybdenum content is determined as corresponding to Moequiv.>=13.8. The total aluminum and zirconium content does not exceed 7.2. The inventive method for heat treatment consists in heating to tbeta<>alpha+beta-(30-70)° C., conditioning during 2-5 hrs. at that temperature, air or water cooling and age-hardening at a temperature ranging from 540° C. to 600° C. during 8-16 hrs. Said alloy has a high volumetric deformability and is used for manufacturing massive large-sized forged and pressed pieces having a high strength level, satisfactory characteristics of plasticity and fracture toughness.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 18.

Claims (3 — 3 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    Titanium-based alloy containing aluminum, vanadium, molybdenum, chromium, iron, zirconium, oxygen and titanium which distinction is that it additionally contains nitrogen with the following proportion of components, % by mass: aluminum

  2. Claim 2Independent Claim

    0-3.6 iron 0.2-0.5

  3. Claim 4Independent Claim

    5-6.0 chromium

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗