Semiconductor device fabrication method
Abstract
During etching of a BARC film, etching gas is used in which O 2 , Cl 2 and He are mixed in appropriate flow volume ratios, and an appropriate ion energy is set. Thus, a selectivity ratio with respect to an underlying film, which is a SiN film, can be sufficiently assured and a pattern is formed uniformly. During etching of a SiN film, etching gas is used in which HBr, CH 4 and He are mixed in appropriate flow volume ratios, and an appropriate ion energy is set. Thus, the form of a pattern is consistent regardless of high- and low-density portions.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 4.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A semiconductor device fabrication method including etching a BARC film disposed with an underlying SiN or polySi film, the etching comprising: dry-etching the BARC film with an etching gas which is formed by mixing a plurality of gases including at least O 2 , Cl 2 and He at predetermined flow volume ratios; and during said dry-etching the BARC film with the etching gas, increasing an etching selectivity ratio of the BARC film relative to the underlying film by increasing the flow volume ratio of O 2 relative to Cl 2 .
- Claim 2Depends on #1
The semiconductor device fabrication method of claim 1 , wherein the flow volume ratio of O 2 relative to Cl 2 is increased to substantially 1.5.
- Claim 3Independent Claim
A semiconductor device fabrication method including etching a BARC film disposed with an underlying SiN or polySi film, t