Solution for ruthenium chemical mechanical planarization
Abstract
A solution for ruthenium chemical mechanical planarization containing a nitric acid and an oxidizer is disclosed. A method of forming ruthenium pattern using a polished ruthenium layer is also disclosed. The disclosed solution improves the polishing speed of ruthenium under low polishing pressure, reduces the dishing of ruthenium and decreases scratches generated in the interlayer insulating film. As a result, the disclosed solution and methods improve the techniques for device isolation and reduction of step coverage.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 12.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A CMP solution for polishing ruthenium comprising a nitric acid and an oxidizer; and wherein the CMP solution is free of abrasives.
- Claim 2Depends on #1
The solution according to claim 1 , wherein a concentration of nitric acid ranges from about 0.01 M to about 10 M.
- Claim 3Depends on #2
The solution according to claim 2 , wherein a concentration of nitric acid ranges from about 0.01 M to about 5 M.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (12 of 12 total)
References Cited — Backward Prior Art (9)
Non-Patent Literature (1)
- Communication from Korean Intellectual Property Office dated Jan. 30, 2004 with translation (4 pages).