Silicon carbide schottky barrier diode and method of making

9Forward Citations (#12244457 Global)
0.4/yrCitation Velocity (#19585465 Global)
1.48Citation PageRank (#23349782 Global)
19Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A Schottky barrier diode and process of making is disclosed. The process forms a metal contact pattern in masked areas on a silicon carbide wafer. A preferred embodiment includes on insulating layer that is etched in the windows of the mask. An inert edge termination is implanted into the wafer beneath the oxide layer and adjacent the metal contacts to improve reliability. A further oxide layer may be added to improve surface resistance to physical damage.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 9.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for the fabrication of a Schottky barrier diode on an SiC wafer, comprising the steps of: (a) forming an insulating layer on the surface of the SiC wafer; (b) placing a mask having a window on an exposed surface of the insulating layer; (c) etching away a portion of the insulating layer corresponding to the window to expose a portion of the SiC wafer therebeneath; (d) while retaining the mask in place, depositing conductive material on the mask and exposed portions of the wafer surface; (e) stripping off the mask so as to leave the conductive material deposited upon the portion of the

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (19)

PatentTitleYearCitations
US 3,412,456 AProduction method of semiconductor devices196832
US 3,445,926 AProduction of semiconductor devices by use of ion beam implantation196911
US 3,567,508 ALow temperature-high vacuum contact formation process197133
US 4,115,120 AMethod of forming thin film patterns by differential pre-baking of resist197841
US 4,448,800 AMethod for the manufacture of semiconductor device using refractory metal in a lift-off step198440
US 4,481,041 AMethod for producing Schottky diodes198414
US 4,558,508 AProcess of making dual well CMOS semiconductor structure with aligned field-dopings using single masking step198548
US 4,599,243 AUse of plasma polymerized organosilicon films in fabrication of lift-off masks198673
US 4,679,303 AMethod of fabricating high density MOSFETs with field aligned channel stops198717
US 4,687,541 ADual deposition single level lift-off process198719
US 4,692,205 ASilicon-containing polyimides as oxygen etch stop and dual dielectric coatings1987146
US 4,745,045 AMethod for improving resolution in microelectronic circuits using photoresist overlayer by using thermally processed polyimide underlayer formed from positive photoresist and polyamic acid198817
US 4,929,567 AMethod of manufacturing a self-aligned GaAs MESFET with T type tungsten gate199022
US 5,006,488 AHigh temperature lift-off process199110
US 5,087,322 ASelective metallization for high temperature semiconductors199213
US 5,270,244 AMethod for forming an oxide-filled trench in silicon carbide199344
US 5,610,098 AN-INP Schottky diode structure and a method of making the same19972
US 5,612,232 AMethod of fabricating semiconductor devices and the devices199735
US 5,635,412 AMethods of fabricating voltage breakdown resistant monocrystalline silicon carbide semiconductor devices199749

Non-Patent Literature (3)

  • Disclosure ID700627-PHA23, B68, U.S. Ser. No. 09/455,633, Filed Dec. 7, 1999.
  • Disclosure ID700627—PHA23, B68, U.S. Ser. No. 09/455,633, Filed Dec. 7, 1999.
  • IBM Technical Disclosure Bulletin NN81102453, Oct. 1981 pp. 2543-2544.*