Patents
US 6,797,560 B2#11553551 Most CitedExpiredUnited States (USPTO)Utility

Method of manufacturing a capacitor having tantalum oxide film as an insulating film

9Forward Citations (#11553551 Global)
0.4/yrCitation Velocity (#19515916 Global)
2.17Citation PageRank (#12779035 Global)
5Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A tantalum oxide film is formed on a lower conductive film by vapor-deposition, and then is treated with active oxygen species. The treated film is annealed at a temperature lower than the crystallization temperature of tantalum oxide by 10 to 80° C. in an inert atmosphere. Subsequently, an upper conductive film is formed on the annealed tantalum oxide film.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 9.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a capacitor having a tantalum oxide film as an insulating film, said method comprising: vapor-phase depositing a tantalum oxide film on a lower electrode comprising a ruthenium film; treating the tantalum oxide film at a temperature of 300 to 500° C. in an atmosphere of active oxygen species; then immediate annealing the tantalum oxide film treated with the active oxygen species, at a temperature of 620 to 690° C., which temperature is lower than a crystallization temperature of tantalum oxide, in an inert atmosphere; and forming an upper electrically conductive film

  2. Claim 2Independent Claim

    A method of manufacturing a capacitor having a tantalum oxide film as an insulating film, said method comprising: vapor-phase depositing a tantalum oxide film

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗