Process for obtaining non thermoprocessable fine powders of homopolymer or modified PTFE
Abstract
A process for obtaining non thermoprocessable fine powders of homopolymer or modified PTFE, comprising the following steps: A) obtaining of the polymer latex under the gel form; B) washing of the polymer gel with acid aqueous solutions or neutral aqueous solutions; C) granulation of the gel washed by mechanical stirring, at a specific power in the range 1.5-10 kW/m 3 , until flotation of the PTFE fine powder, and separation of the floated fine powder; D) drying in an aerated oven of the floated fine powder at a drying temperature in the range 90° C.-160° C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 15.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process to obtain non-thermoprocessable fine powders of photopolymer or modified PTFE, comprising the following steps: A) obtaining of the polymer latex under the gel form; B) washing of the polymer gel with acid aqueous solutions or neutral aqueous solutions, having a pH from 0.5 to 7 C) granulation of the washed gel by mechanical stirring, at a specific power in the range 1.5-10 kW/m3, until flotation of the PTFE fine powder, and separation of the floated fine powder; D) drying in an aerated oven of the floated fine powder at a drying temperature in the range 90° C.-160° C.
- Claim 2Depends on #1
A process according to claim 1 , carried out in batch or in a continuous way.
- Claim 3Depends on #2
A process according to claim 2 , wherein the dilution is from 8 to 20% by weight of PTFE, the temperature of the di