Patents
US 6,784,504 B2#6490355 Most CitedExpiredUnited States (USPTO)Utility

Methods for forming rough ruthenium-containing layers and structures/methods using same

15Forward Citations (#6490355 Global)
0.7/yrCitation Velocity (#11204361 Global)
1.90Citation PageRank (#15738256 Global)
47Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method for forming a rough ruthenium-containing layer on the surface of a substrate assembly includes providing a ruthenium-containing precursor into the reaction chamber. A rough ruthenium layer may be deposited on the surface of the substrate assembly at a rate of about 100 Å/minute to about 500 Å/minute using the ruthenium-containing precursor. Further, a rough ruthenium oxide layer may be formed by providing a ruthenium-containing precursor and an oxygen-containing precursor into the reaction chamber to deposit the rough ruthenium oxide layer on the surface of the substrate assembly at a rate of about 100 Å/minute to about 1200 Å/minute. An anneal of the layers may be performed to further increase the roughness. In addition, conductive structures including a rough ruthenium layer or a rough ruthenium oxide layer are provided. Such layers may be used in conjunction with non-rough ruthenium and/or non-rough ruthenium oxide layers to form conductive structures. For example, such structures may be part of a capacitor structure, e.g., bottom electrode of a capacitor.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 47 · Forward citations: 15.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A conductive structure comprising at least a rough ruthenium layer, wherein a surface of the rough ruthenium layer has a surface area greater than about 1.2 times a surface area of a completely smooth surface having a substantially identical shape as the surface of the rough ruthenium layer.

  2. Claim 2Depends on #1

    The conductive structure of claim 1 , wherein the surface of the rough ruthenium layer has a surface area greater than about 1.5 times the surface area of the completely smooth surface having the substantially identical shape as the surface of the rough ruthenium layer.

  3. Claim 3Depends on #1

    The conductive structure of claim 1 , wherein an RMS roughness of the surface of the rough ruthenium layer is in a range of about 50 Å to about 600 Å.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (47)

Non-Patent Literature (5)

  • Anderson et al., "Carborane Complexes of Ruthenium: A Convenient Synthesis of [Ru(CO) of-7,8-C B.H )]and a Study of Reactions of This Completx" Organometallics, 14, 3516-3526 (1995).
  • Aoyama et al., "Chemical Vapor Deposition of Ru and Its Application in (Ba.Sr)TiO Capacitors for Future Dynamic Random Access Memories," Jpn. J. Appl. Phys. 38:2194-2199 (1999).
  • Bau et al., "Low-Temperature growth and orientalinal control in RuO, thin films by metal-organic chemical vapor deposition", Thin Solid Films, 310, 75-80 (1997).
  • Bennett et al., "Mono-olefin Chelate Complexes of Iron(0) and Ruthenium(0) with an Olefinic Tertiary Phosphane," J. Chem. Soc. D.. 7. 341 342 (1971).
  • Cowles et al., "Relative Reactivity of Co-ordinated Ligands inthe Dierryltricarbonyl-ruthenium Cation. [adienyl RutCO.]," Chemical Commun.. 392 (1969).