Patents
US 6,784,094 B2#8385534 Most CitedExpiredUnited States (USPTO)Utility

Anti-reflective coatings and methods for forming and using same

12Forward Citations (#8385534 Global)
0.6/yrCitation Velocity (#14525170 Global)
2.37Citation PageRank (#11111658 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

An anti-reflective coating material layer is provided that has a relatively high etch rate such that it can be removed simultaneously with the cleaning of a defined opening in a relatively short period of time without affecting the critical dimensions of the opening. A method of forming such a layer includes providing a substrate assembly surface and using a gas mixture of at least a silicon containing precursor, a nitrogen containing precursor, and an oxygen containing precursor. The layer is formed at a temperature in the range of about 50° C. to about 600° C. Generally, the anti-reflective coating material layer deposited is Si x O y N z :H, where x is in the range of about 0.39 to about 0.65, y is in the range of about 0.02 to about 0.56, z is in the range of about 0.05 to about 0.33, and where the atomic percentage of hydrogen in the inorganic anti-reflective coating material layer is in the range of about 10 atomic percent to about 40 atomic percent. The total SiH 4 flow is generally in the range of about 80 sccm to about 400 sccm. The gas mixture may include SiH 4 and N 2 O, where the ratio of SiH 4 :N 2 O is in the range of about 0.25 to 0.60. The inorganic anti-reflective

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 12.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for use in fabrication of integrated circuits, the method comprising: providing a substrate assembly having an opening defined therein by at least one surface of BPSG, wherein the opening is defined using an inorganic anti-reflective coating material layer with at least a portion of the anti-reflective coating material layer remaining on the substrate assembly after the opening is defined; and completely removing the inorganic anti-reflective coating material layer with less than about 100 angstroms of the at least one surface of BPSG being removed during cleaning of the opening.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the inorganic anti-reflective coating material layer has a thickness in the range of about 100 Å to about 1000 Å.

  3. Claim 3Depends on #2

    The method of claim 2 , wherein completely removing th

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 4,352,724 AMethod of manufacturing a semiconductor device198289
US 4,363,868 AProcess of producing semiconductor devices by forming a silicon oxynitride layer by a plasma CVD technique which is employed in a selective oxidation process198232
US 4,451,969 AMethod of fabricating solar cells1984105
US 4,532,022 AProcess of producing a semiconductor device198536
JP S6159820 AManufacture of semiconductor device—16
US 4,764,248 ARapid thermal nitridized oxide locos process198883
US 4,921,572 AEtchant solutions containing hydrogen fluoride and a polyammonium fluoride salt199070
JP H03101147 AManufacture of semiconductor device—23
US 5,124,780 AConductive contact plug and a method of forming a conductive contact plug in an integrated circuit using laser planarization1992107
US 5,194,777 AMethod for fabricating electroluminescence display device and electroluminescence display device199313
US 5,216,542 ACoating, composed of an optically effective layer system, for substrates, whereby the layer system has a high anti-reflective effect, and method for the manufacturing of the coating199386
US 5,270,241 AOptimized container stacked capacitor DRAM cell utilizing sacrificial oxide deposition and chemical mechanical polishing1993232
US 5,374,585 AProcess for forming field isolation199438
US 5,392,189 ACapacitor compatible with high dielectric constant materials having two independent insulative layers and the method for forming same1995333
US 5,418,019 AMethod for low temperature plasma enhanced chemical vapor deposition (PECVD) of an oxide and nitride antireflection coating on silicon199554
US 5,441,914 AMethod of forming conductive interconnect structure199578
JP H0831812 AFormation of element-isolating area for semiconductor device—11
JP H0831811 AMethod for forming element isolation area of semiconductor device—14

Non-Patent Literature (5)

  • Bencher et al., "Dielectric antireflective coatings for DUV lithography," Solid State Technology, 1997;114:109, 111-112, and 114.
  • Dammel et al., "Dependence Of Optical Contants Of AZ(R)BARLi(TM) Bottom Coating On Bake Conditions," SPIE; 1997; 3049:963-973.
  • Dammel et al., "Dependence Of Optical Contants Of AZ®BARLi™ Bottom Coating On Bake Conditions," SPIE; 1997; 3049:963-973.
  • Gocho et al., "CVD Method of Anti-Reflective Layer Film for Excimer Laser Lithography," Int. Conf. On Solid State Devices & Materials, Makuhari, Aug. 29-Sep. 1; 1993:570-572.
  • Heavens, Optical Properties of Thin Solid Films, Dover Publications, Inc., New York, NY 1955:48-49.