Patents
US 6,783,442 B2#12760891 Most CitedExpiredUnited States (USPTO)Utility

Nickel-diamond-coated saw wire with improved anchoring of the diamond particles

8Forward Citations (#12760891 Global)
0.4/yrCitation Velocity (#21823701 Global)
2.39Citation PageRank (#10897935 Global)
20Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The invention relates to a saw wire consisting essentially of a steel wire, an intermediate layer and a metallic binding phase into which diamond grains with an average diameter of 10 to 50 micrometers are inserted, characterized in that the metallic binding phase has a hardness of between 600 and 1100 HV 0.1 and consists of an inner layer and an outer layer which are arranged concentrically around the steel wire provided with the intermediate layer. The inner layer has a thickness of approximately between 10 and 25% of the average diamond grain diameter, while the thickness of the outer layer is such that the overall thickness of the metallic binding phase is 45-55% of the average diamond grain diameter and the diamond grains have an average interval of not more than 5 times their average diameter. Other fine particles with an average diameter of 1 to 6 micrometers are located between the diamond grains with an average diameter of 10 to 50 micrometers.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 8.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A saw wire with a high resistance to wear when sawing hard materials, comprising a steel wire, an intermediate layer and a metallic binder phase of nickel deposited without external current in which diamond grains, with a mean diameter of 10 to 50 mm μm are embedded, the immediate layer being undamaged and free of diamond grains and serving both to prevent hydrogen embrittlement of the wire and to ensure adhesive strength of the metallic binder phase, wherein the metallic binder phase has a hardness of between 600 and 1100 HV 0.1 and comprises an inner layer and an outer layer, which are arran

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • (Enc) US 091332,722 (Lukschandel et al).
  • English Derwent Abstract AN 1978-G0800A [31] Corresp. to DE 2805745A1.
  • English Derwent Abstract AN 1999-012305 [02] Coresp. to DE 19822265A1.
  • English Derwent Abstract AN 2000-17359 [16] Corresp-to DE 19839091 A1.
  • Patent Abstracts of Japan Pub. # 09001455 A (encl.).