Coagulation process of PTFE fine powders
Abstract
A continuous coagulation process of PTFE or modified PTFE fine powders, comprising: a1) dilution in a lift of a PTFE latex up to a concentration from 5 to 25% w/w of PTFE, and optional filtration of the obtained diluted latex, b1) latex pressurization in the lift by an inert gas, preferably air, until a relative pressure, related to the atmospheric pressure, in the range 3-40 kg/cm 2 (0.3-4 MPa), c1) addition of an acid electrolyte solution, d1) latex flowing from the mixer through a capillary tube under turbulent flow conditions, e1) granulation (coagulation) of the gel obtained in step d1) by mechanical stirring with a specific power from 1.5 to 10 kW/m 3 , maintaining the stirring until fine powder flotation, f1) separation of the underlying water from the fine powder.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 14.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A continuous coagulation process of PTFE or modified PTFE fine powders, comprising: a1) dilution in a lift of a PTFE latex obtained from the polymerization in dispersion (emulsion) to a concentration from 5 to 25% w/w of PTFE, or modified PTFE; and optional filtration of the obtained diluted latex; b1) latex pressurization in the lift by an inert gas, up to a relative pressure, referred to the atmospheric pressure, in the range 3-40 kg/cm 2 (0.3-4 MPa); c1) addition of an acid electrolyte solution, to the PTFE latex, in a in-line mixer, so that the pH is from 1 to 4; d1) latex flowing from th
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗