Patents
US 6,780,773 B2#19356163 Most CitedExpiredUnited States (USPTO)Utility

Method of chemical mechanical polishing with high throughput and low dishing

5Forward Citations (#19356163 Global)
0.2/yrCitation Velocity (#30679461 Global)
2.20Citation PageRank (#12468092 Global)
50Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Method and apparatus are provided for polishing conductive materials with low dishing of features and reduced or minimal remaining residues. In one aspect, a method is provided for processing a substrate by polishing the substrate to remove bulk conductive material and polishing the substrate by a ratio of carrier head rotational speed to platen rotational speed of between about 2:1 and about 3:1 to remove residual conductive material. In another aspect, a method is provided for processing a substrate including polishing the substrate at a first relative linear velocity between about 600 mm/second and about 1900 mm/second at the center of the substrate, and polishing the substrate at a second relative linear velocity between about 100 mm/second and about 550 mm/second at the center of the substrate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 5.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for processing a substrate, comprising: providing a substrate having a conductive material disposed thereon to a polishing apparatus having one or more rotational carrier heads and one or more rotatable platens; polishing the substrate at a first relative linear velocity between about 600 mm/second and about 1900 mm/second at the center of the substrate; and polishing the substrate at a second relative linear velocity between about 100 mm/second and about 550 mm/second at the center of the substrate and at a ratio of carrier head rotational speed to platen rotational speed of between

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the first relative linear velocity is between about 1000 mm/second and about 1200 mm/second at the center of the substrate.

  3. Claim 3Independent Claim

    The met

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 5,234,867 AMethod for planarizing semiconductor wafers with a non-circular polishing pad1993238
US 5,302,233 AMethod for shaping features of a semiconductor structure using chemical mechanical planarization (CMP)1994201
US 5,627,110 AMethod for eliminating window mask process in the fabrication of a semiconductor wafer when chemical-mechanical polish planarization is used199747
US 5,676,567 AInternal/external modular interface199717
US 5,733,177 AProcess of polishing wafers199842
US 5,738,574 AContinuous processing system for chemical mechanical polishing1998733
US 5,786,275 AProcess of fabricating wiring structure having metal plug twice polished under different conditions199840
US 5,827,781 APlanarization slurry including a dispersant and method of using same199876
US 5,853,604 AMethod of planarizing an insulating layer in a semiconductor device199814
US 5,876,266 APolishing pad with controlled release of desired micro-encapsulated polishing agents199977
US 5,897,426 AChemical mechanical polishing with multiple polishing pads1999157
US 5,952,243 ARemoval rate behavior of spin-on dielectrics with chemical mechanical polish199952
US 5,976,979 ASequential oxygen plasma treatment and chemical mechanical polish (CMP) planarizing method for forming planarized low dielectric constant dielectric layer199941
US 5,985,748 AMethod of making a semiconductor device using chemical-mechanical polishing having a combination-step process199995
US 6,001,730 AChemical mechanical polishing (CMP) slurry for polishing copper interconnects which use tantalum-based barrier layers1999287
US 6,024,630 AFluid-pressure regulated wafer polishing head2000183
WO 0,024,842 A1A chemical mechanical polishing slurry system having an activator solution—43
US 6,068,879 AUse of corrosion inhibiting compounds to inhibit corrosion of metal plugs in chemical-mechanical polishing2000117
EP 1,006,166 A1Polishing composition and polishing method employing it—45
EP 1,011,131 A1Methods for enhancing the metal removal rate during the chemical-mechanical polishing process of a semiconductor—19
US 6,083,840 ASlurry compositions and method for the chemical-mechanical polishing of copper and copper alloys2000247
US 6,113,465 AMethod and apparatus for improving die planarity and global uniformity of semiconductor wafers in a chemical mechanical polishing context200039
US 6,114,247 APolishing cloth for use in a CMP process and a surface treatment thereof200011
US 6,117,775 APolishing method2000228
US 6,121,144 ALow temperature chemical mechanical polishing of dielectric materials200048

Non-Patent Literature (2)

  • European Search Report for EP 00 31 1569 dated Nov. 12, 2003 (AMAT/3786.EP).
  • U.S. patent application for 09/469,709 filed on Dec. 21, 1999 (AMAT/3786.Y1).