Patents
US 6,780,261 B2#7876335 Most CitedExpiredUnited States (USPTO)Utility

Method of manufacturing an implantable stent having improved mechanical properties

13Forward Citations (#7876335 Global)
0.6/yrCitation Velocity (#13584323 Global)
1.51Citation PageRank (#22651504 Global)
8Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A metallurgical process for producing a metallic implantable medical device, such as a stent, in a condition wherein the metallic alloy of the device has improved mechanical properties. The starting material is formed into an oversized tube which is drawn to finished outer diameter. The drawing process cold works the tube to produce a material having a high dislocation density and a yield strength that is above approximately 125 ksi. Next, the drawn tube is heat treated at a temperature of approximately one-half the absolute melting temperature of the alloy. The heat treatment causes dislocations to rearrange, forming sub-grains and re-crystallization of the grain structure. Upon cooling, a material is obtained having a yield strength between approximately 45-70 ksi and an elongation exceeding 40 percent. The material also has good resistance to fatigue fracture due to the fine grains and sub-grains that are established during the heat treatment.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 13.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for manufacturing a stent assembly having improved mechanical properties, the process comprising the steps of: first, providing an oversized tubular member of an alloy; second, drawing the oversized tubular member to a smaller outer diameter and thinner wall to the tube to a yield strength above approximately 125 ksi; and third, heating the cold-worked tube to a first temperature for a sufficient time, followed by cooling to produce a material having a yield strength between about 40 ksi and about 70 ksi, and an elongation above 40 percent.

  2. Claim 2Depends on #1

    The process as recited in claim 1 , wherein the first temperature is about one-half the absolute melting temperature of said alloy.

  3. Claim 3Depends on #1

    The process as recited in claim 1 , wherein the first temperature is between about 40 percent of t

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • International Search Report from PCT/US 03/20212.