Abstract
A process is described for producing an aluminum alloy sheet having excellent bendability for use in forming panels for automobiles. An aluminum alloy containing 0.50 to 0.75 by weight Mg, 0.7 to 0.85% by weight Si, 0.1 to 0.3% by weight Fe, 0.15 to 0.35% by weight Mn, and the balance Al and incidental impurities, is used and is semi-continuously cast into ingot. The cast alloy ingot is subjected to hot rolling and cold rolling, followed by solution heat treatment of the formed sheet. The heat treated sheet is quenched to a temperature of about 60-120° C. and the sheet is then coiled. This coil is then pre-aged by slowly cooling the coil from an initial temperature of about 60-120° C. to room temperature at a cooling rate of less than 10° C./hr.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 23.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process of producing an aluminum alloy sheet having excellent bendability for use in forming panels for automobiles, the process comprising the steps of: semi-continuously casting an aluminum alloy comprising 0.50 to 0.75% by weight Mg, 0.7 to 0.85% by weight Si, 0.1 to 0.3% by weight Fe, 0.15 to 0.35% by weight Mn, 0 to 0.4% by weight Cu, and the balance Al and incidental impurities, subjecting the cast alloy ingot to hot rolling and cold rolling, followed by solution heat treatment of the formed sheet, quenching the heat treated sheet to a temperature of about 60-120° C. and coiling the sh
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 23 total)
References Cited — Backward Prior Art (16)
Non-Patent Literature (1)
- "ASM Specialty Handbook: Aluminum and Aluminum Alloys", ASM International (1993), p 529.