Abstract

The present invention provides an effective method for mechanically removing iron oxide films formed on the surfaces of a hot rolled steel strip with a high temperature. The method comprises the steps of: maintaining a steel strip coil at a high temperature of 400° C. or more until the phase transformation is completed, after hot rolling; water-cooling the steel strip coil at a speed of at least 50° C./sec to 100° C. or less while uncoiling the coil; correcting the shape of the steel strip using a correction rolling mill; removing oxide films formed on surfaces of the shape-corrected steel strip by injecting water jets to the surface; and drying the steel strip free of oxide films and winding the steel strip. Also, the present invention provides an apparatus for carrying out this method.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 9.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing a hot rolled steel strip free of oxide films comprising the steps of: maintaining a steel strip coil at a high temperature as it is at a temperature of 400° C. or more until the phase transformation is completed, after hot rolling; water-cooling the steel strip coil at a speed of at least 50° C./sec to 100° C. or less while uncoiling the coil; correcting the shape of the steel strip using a correction rolling mill; removing oxide films formed on surfaces of the shape-corrected steel strip by injecting water jets to the surface; and drying the steel strip free of oxid

  2. Claim 2Depends on #1

    The method as set forth in claim 1 , wherein the steel strip coil is cooled to a temperature of 60 to 100° C. at the water-cooling step.