Abstract
Process for making free rise or slabstock flexible polyurethane foams with high resilience using diphenylmethane diisocyanate and a polyol composition comprising: (a) a polyoxyethylene-polyoxypropylene-polyol, having an average nominal hydroxyl functionality of 2-8, an average equivalent weight of 1000-4000 and containing 10-25% by weight of oxyethylene groups; (b) 3 to 8 parts by weight of water as the sole blowing agent or optionally together with CO2 as the sole blowing agents; and (c) 2 to 20, preferably 2 to 10 parts by weight of a polyether polyol having an average nominal hydroxyl functionality of 2-6, an average equivalent weight of 200-600 and containing at least 60% by weight of oxyethylene groups; and optionally (d) up to 30 and preferably 2-25 parts by weight of particulate material which is dispersed in said polyol composition; the amounts of (b)(ii) to (b)(iv) being calculated per 100 parts by weight of (b)(i); and optionally (e) auxiliaries and additives.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 41 · Forward citations: 10.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for preparing a free rise or slabstock flexible polyurethane foam with a free rise density of 20 to 35 kg/m 3 and a high resilience at an NCO index of 70-120 by reacting: (a) a polyisocyanate composition having an isocyanate functionality below 2.15 and consisting of diphenylmethane diisocyanate and optionally homologues thereof having an isocyanate functionality of 3 or more, the amount of diphenylmethane diisocyanate being 81 to 100% by weight calculated on the amount of diphenylmethane diisocyanates and homologues, and the diphenylmethane diisocyanate comprising 40-60% by weight,
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗