Abstract

Ions are implanted into a resist pattern for forming a wiring pattern. Argon is employed as the ion species, for performing ion implantation under 50 keV at 1x10<16>/cm<2>. Due to the ion implantation, the thickness of the resist pattern contracts to about 334 nm, i.e., about 75% of the thickness of 445 nm before ion implantation, while the composition of the resist pattern changes for improving resistance against etching for a silicon nitride film and a polysilicon layer. Thus obtained is a method of manufacturing a semiconductor device capable of suppressing critical dimension shift density difference (difference between a critical dimension shift on a rough region having a relatively large space width and that on a dense region having a relatively small space width).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 19.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a semiconductor device, comprising steps of: (1) predetermining a first thickness of a first resist film and an ion implantation level that will cause the first thickness to contract to a second thickness; (a) forming an etching object on a semiconductor substrate; (b) forming said first resist film with said first thickness on said etching object; (c) patterning said first resist film to obtain a first resist pattern; (d) performing ion implantation into said first resist pattern with said ion implantation level set so that the first predetermined thickness contracts

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 19 total)

PatentTitleYearCitations
US 6,905,811 B2Method to form reduced dimension pattern with good edge roughness20055
US 2009253263 A1Method for fabricating semiconductor device capable of decreasing critical dimension in peripheral region—2
US 2004180528 A1Method of forming a dual-layer resist and application thereof—6
US 7,923,375 B2Method for manufacturing semiconductor device20111
US 2010102255 A1Method of transferring pattern of reticle, computer readable storage medium, and method of manufacturing device—4
US 6,908,854 B2Method of forming a dual-layer resist and application thereof20058
US 7,563,721 B2Method for fabricating semiconductor device capable of decreasing critical dimension in peripheral region20091
US 2005287809 A1Method for fabricating semiconductor device capable of decreasing critical dimension in peripheral region—12
US 11,579,537 B2Pattern inspection method and photomask fabrication method20230
US 2009233448 A1Lithography resolution improving method—19
US 7,803,710 B2Method for fabricating semiconductor device capable of decreasing critical dimension in peripheral region20100
US 2003114012 A1Method for forming pattern using argon fluoride photolithography—8
US 8,049,191 B2Method of transferring pattern of reticle, computer readable storage medium, and method of manufacturing device20112
US 8,658,051 B2Lithography resolution improving method20140
US 2007184664 A1Method for fabricating semiconductor device capable of decreasing critical dimension in peripheral region—5

Non-Patent Literature (3)

  • U.S. patent application Ser. No. 09/413,723, filed Oct. 7, 1999, allowed.
  • U.S. patent application Ser. No. 09/915,396, filed Jul. 27, 2001, pending.
  • Wolf et al., Silicon Processing for the VLSI Era, vol. 1, 1986, pp. 181-182, 191-195, 407-408.*