Patents
US 6,773,487 B2#33306601 Most CitedExpiredUnited States (USPTO)Utility

Process for refining silver bullion with gold separation

3Forward Citations (#33306601 Global)
0.1/yrCitation Velocity (#39723053 Global)
1.05Citation PageRank (#39096090 Global)
10Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A process is disclosed for refining silver bullion, i.e. raw silver containing generally more than 90% silver besides Se, Pb, Au, Cu and platinum group metals (PGM) as main impurities. The process comprises: optionally removing Se as gaseous SeO 2 from the molten metallic phase by injecting air, which is preferably O 2 enriched, into the metallic phase at a preferred bath temperature of 1000-1100° C.; optionally slagging off the Pb by contacting the molten metallic phase with a silica and borax based flux at a preferred bath temperature of 1000-1150° C.; granulating the molten metallic phase in water, thereby forming Ag rich granules; leaching the Ag rich granules with HNO 3 at a temperature above 50° C., preferably in an O 2 enriched atmosphere, followed by filtration, thereby separating an Au bearing residue from an Ag rich liquor; heating the Ag rich liquor, thereby evaporating H 2 O and forming an AgNO 3 bearing melt; maintaining the AgNO 3 bearing melt at a temperature of 220-350° C. for at least 15 minutes, thereby forming a mixture of a purified AgNO 3 and of a denitration residue containing essentially all the PGM as oxides; separating the purified AgNO 3 from the denitrati

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 3.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for refining impure silver bullion containing metals from the group consisting of Pb, Se, Cu, Au and platinum group metals as impurities, comprising: leaching the silver bullion with HNO 3 at a temperature above 50° C., followed by filtration, thereby separating a Au bearing residue from an Ag rich liquor; heating the Ag rich liquor, thereby evaporating H 2 O and forming an AgNO 3 bearing melt; maintaining the AgNO 3 bearing melt at a temperature of 300-350° C. for at least 15 minutes, thereby forming a mixture of a purified AgNO 3 and a denitration residue containing essentially

  2. Claim 2Depends on #1

    The process according to claim 1 , wherein said leaching the silver bullion takes place

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Copy of International Search Report from related PCT/EP01/00613 mailed Jun. 13, 2001, 3 pages.