Fibers and webs capable of high speed solid state deformation
Abstract
The present invention relates to an intermediate web comprising of high glass transition polymer fibers. The fibers are spun at low to moderate speeds and have a relative crystallinity of from 10% to 75% of the maximum achievable crystallinity. The intermediate web is a low crystallinity web that exhibits shrinkage of more than 30% and elongation to break of more than 80% at high strain rates. This web can be heat treated to reduce shrinkage to less than 15% while the web is capable of at least about 60% elongation at a strain rate of at least about 50 second −1 .
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 36.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
An intermediate web comprising high glass transition polymer fibers, said fibers having a relative crystallinity of from about 10% to about 75% of the maximum achievable crystallinity, and said fibers being from 5 to 30 microns in diameter, wherein said web is capable of: a. at least about 80% elongation at a strain rate of at least about 50 second −1 and b. shrinkage of greater than 15%.
- Claim 2Depends on #1
The web of claim 1 wherein the fibers are comprised of bicomponent cross sectional segments with a majority section comprised of a crystallizable high glass transition polymer having a maximum achievable absolute crystallinity of from about 15% to about 60%.
- Claim 3Depends on #1
The web of claim 1 wherein the high glass transition polymer fibers comprise polyethylene terephthalate, polytrimethylene terephthalate, or po
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗