Thin-film transistors formed on a flexible substrate
Abstract
A method for is provided forming a thin-film transistor (TFT) on a flexible substrate. The method comprises: supplying a metal foil substrate such as titanium (Ti), Inconel alloy, stainless steel, or Kovar, having a thickness in the range of 10 to 500 microns; depositing and annealing amorphous silicon to form polycrystalline silicon; and, thermally growing a gate insulation film overlying the polycrystalline. The silicon annealing process can be conducted at a temperature greater than 700 degrees C. using a solid-phase crystallization (SPC) annealing process. Thermally growing a gate insulation film includes: forming a polycrystalline silicon layer having a thickness in the range of 10 to 100 nanometers (nm); and, thermally oxidizing the film at temperature in the range of 900 to 1150 degrees for a period of time in the range of 2 to 60 minutes. Alternately, a plasma oxide layer is deposited over a thinner thermally oxidized layer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 36.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A thin-film transistor (TFT) on a flexible substrate comprising: a metal foil substrate with a surface; an electrical isolation layer overlying the metal foil substrate surface; drain, source, and channel regions formed from polycrystalline silicon overlying the electrical isolation layer; a gate insulation oxide film overlying the polycrystalline silicon having an index of refraction in the range of 1.4 to 1.6; and, a gate overlying the gate insulation oxide layer.
- Claim 2Depends on #1
The TFT of claim 1 wherein the metal foil substrate has a thickness in the range of 10 to 500 microns.
- Claim 3Depends on #2
The TFT of claim 2 wherein the metal foil substrate has a thickness in the range of 50 to 250 microns.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 36 total)
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 6,329,226 B1 | Method for fabricating a thin-film transistor | 2001 | 70 |
| US 6,642,092 B1 | Thin-film transistors formed on a metal foil substrate | 2003 | 59 |