An object of the invention is to provide a low temperature fired porcelain having an optimum firing temperature not higher than 1000° C. a reduced dielectric constant ∈ r, an improved quality coefficient and a low incidence of cracks. The invention provides a low temperature-fired porcelain comprising a barium component in a calculated amount of 10 to 64 weight percent when calculated as BaO, a silicon component in a calculated amount of 20 to 80 weight percent when calculated as SiO2, an aluminum component in a calculated amount of 0.1 to 20 weight percent when calculated as Al2O3, a boron component in a calculated amount of 0.3 to 1.0 weight percent when calculated as B2O3 a zinc component in a calculated amount of 0.5 to 20 weight percent when calculated as ZnO, and a bismuth component in a calculated amount of not higher than 20 weight percent when calculated as Bi2O3.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 8.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A low temperature-fired porcelain comprising a barium component in an amount of 10 to 64 weight percent when calculated as BaO, a silicon component in an amount of 20 to 80 weight percent when calculated as SiO 2 , an aluminum component in an amount of 0.1 to 20 weight percent when calculated as Al 2 O 3 , a boron component in an amount of 0.3 to 1.0 weight percent when calculated as B 2 O 3 , a zinc component in an amount of 0.5 to 20 weight percent when calculated as ZnO, and a bismuth component in an amount of 0.1 to 20 weight percent when calculated as Bi 2 O 3 .

  2. Claim 2Depends on #1

    The porcelain of claim 1 , comprising said barium component in an amount of not higher than 60 weight percent when calculated as BaO.

  3. Claim 3Depends on #1

    The porcelain of claim 1 , comprising said silicon component in an amount of 30 to 65 weight percent when