Method of producing lithium aluminosilicate ceramics

4Forward Citations (#24001150 Global)
0.2/yrCitation Velocity (#35205274 Global)
1.51Citation PageRank (#22705001 Global)
7Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of producing lithium aluminosilicate (LAS) ceramics, which uses a mixing powder of lithium carbonate, aluminum oxide, and silicon oxide as a raw material powder. After being mixed by ball milling and baked dry, the raw material powder is processed with a calcinations process such that the raw material powder becomes a precursor. The precursor is then pressed into the green ceramic. Significantly, the high heat conducting metal sheets are tightly attached above and below the surfaces of the ceramic during sinter and heat-treatment processes. A solid-state sinter process is performed with the green ceramic. Next, the ceramic is treated with a proper heat-treatment process. Since the top and bottom surfaces of the ceramic are capped with the high heat conducting metal, the ceramics are uniformly heated during all the heating processes. The ceramics of this invention exhibit more uniform properties and stable structure, which allow them to be used as temperature compensation components and athermal products.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 4.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of producing LAS ceramics comprising: providing lithium carbonate, aluminum oxide, and silicon oxide as a raw material powder, mixing, grinding, and then drying the raw material powder; performing a calcinations process on the raw material powder to form a precursor; pressing the precursor into a green ceramic; attaching high thermal conducting metal sheets above and below surfaces of the green ceramic; performing a sinter process to turn the green ceramic into ceramic; and, performing a heat treatment process on the ceramic.

  2. Claim 2Depends on #1

    The method of producing LAS ceramics of claim 1 , wherein the mixing and grinding are performed by ball milling.

  3. Claim 3Depends on #1

    The method of producing LAS ceramics of claim 1 , wherein the lithium carbonate, aluminum oxide a